MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
China-Yixing Longly Refractories Slab SiC
Categories: Ceramic; Carbide

Material Notes: SiC series products of SiC shelf boards, SiC pillars, SiC slab, SiC seggar kiln furniture, are formed using high-quality silicon carbide materials and high temperature binders by tons of high-vibration or hydraulic machine to suppress, high-temperature shuttle kiln firing; products performance and stability excellent, thermal shock good, oxidation resistance good, wear resistance excellent, heat-shock excellent, not slag off, long service life. The appearance of products formed, smooth, high-volume density, good thermal conductivity, energy-saving effect significant.

Applications: Widely used in a variety of tunnel kiln, roller kiln, shuttle kiln production of sanitary ceramics, daily-use ceramics, art ceramics, magnetic materials, powder metallurgy, electrical porcelain, industrial ceramics, as well as refractory products, such as the firing

Information Provided by China Yixing Longly Refractories Co. Ltd

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.60 - 2.70 g/cc
Porosity 15 - 16 %Apparent
 
Mechanical PropertiesOriginal ValueComments
Flexural Strength >= 480 MPacold bending
 >= 500 MPahigh temp bending
Compressive Strength >= 800 MPaAmbient
 
Thermal PropertiesOriginal ValueComments
CTE, linear 2.60 µm/m-°CVolumetric thermal expansion
Thermal Conductivity 16.5 - 17.5 W/m-K
Maximum Service Temperature, Air >= 1450 °C
 
Component Elements PropertiesOriginal ValueComments
SiC >= 85 %
 
Descriptive Properties
Refractoriness (°C)>1400Under load temperature, 0.2 MPa, 0.6%
Thermal Shock Resistance Times501100°C water cooling

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Inhance Fluoro-Seal INHANCE® Si-8220 Polymer Alloy
Inhance Fluoro-Seal INHANCE® Si-8900 Polymer Alloy
Silicon Carbide, Alpha SiC
Silicon Carbide, CVD
Silicon Carbide, sublimed

CYXLR012 / 99314

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.