MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
M. Holland Company MTEGRITY™ CP850 Polypropylene Impact Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes:
  • Impact copolymer
  • Fast production cycle
  • High flow
  • High stiffness

Applications:

  • Containers
  • Household goods
  • Thin-walled parts

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccASTM D1505
Melt Flow 50 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 3900 psiASTM D638
Elongation at Yield 6.0 %ASTM D638
Flexural Modulus 190000 psiASTM D790
Izod Impact, Notched 1.50 ft-lb/in73°F; ASTM D256
 
Descriptive Properties
FormsPellets
Processing MethodsInjection molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Pro-fax™ SC973 Polypropylene Copolymer
Total PPC 4944WZ Polypropylene, Impact Copolymer
ExxonMobil PP7555KNE2 Polypropylene Impact Copolymer
ExxonMobil PP7505KNE2 Polypropylene Homopolymer
LyondellBasell Pro-fax 6524 Polypropylene Homopolymer, Heat- and Extraction-Resistant

PMH111 / 53035

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.