MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

(Viewing data as-entered. Click here to return)
Process Technologies Inc BUNA-N Sanitary Gasket
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: BUNA-N should be considered for use with oils and animal fats. This is a food grade and 3A approved that has good compression set characteristics. BUNA-N does have a limited temperature range which precludes its use in many applications. This material does not meet USP Class VI.

Information provided by Process Technologies Inc

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 93.33 °C
Minimum Service Temperature, Air -34.44 °C
 
Compliance PropertiesOriginal ValueComments
USP Class VI Yes
 
Descriptive Properties
ColorBlack
 Blue
 Green
 Red
 White
 Yellow
Compatibility for ChemicalsAcetoneNot Recommended
 AmmoniaGood
 Hydrochloric AcidNot Recommended
 Hydrofluoric AcidNot Recommended
 Hydrogen PeroxideGood
 Isopropyl AlcoholGood
 Nitric AcidNot Recommended
 Phosphoric AcidGood
 Sodium HydroxideGood
 Sodium HypochloriteGood
 Steam to 400ºF (204ºC)Not Recommended
 Sulfuric AcidLimited

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Nitrile Rubber (NBR, Acrylonitrile-Butadiene Rubber)
Synthos BUNA™ SB 1723 Schkopau Cold Polymerized Emulsion Styrene Butadiene Rubber (E-SBR)
A. Schulman Diamond ABS 3501 Black 1302 Injection Molding Grade
A. Schulman Diamond ABS 3500 Natural 1050
A. Schulman Diamond ABS 2510

PPTI04 / 138116

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.