MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
3M Scotch-Weld™ EC-2815 B/A FR Epoxy Adhesive
Categories: Polymer; Thermoset; Epoxy

Material Notes: 3M Scotch-Weld Epoxy Adhesive EC-2815 B/A FR is a two-component epoxy adhesive with cure at room temperature or with additional heat to form a tough, impact-resistant bond. It has excellent adhesion to many metal, composite, and plastic substrates. The cured material meets the 14 CFR 25.853 (a) before and subsequent to environmental conditioning. Scotch-Weld EC-2815 B/A FR Adhesive is a non-sag, white adhesive that is designed for structural bonding of metal and composite structures and insert bonding.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.10 - 1.30 g/ccUncured, Part A
 1.20 - 1.40 g/ccCured
 1.30 - 1.50 g/ccUncured, Part B
Solids Content 100 %Part B
 100 %Part A
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 56.5 MPacured for 16 hrs at 21-27°C + post cured for 1 hrs at 82°C; ASTM D638-10
Elongation at Break 3.4 %cured for 16 hrs at 21-27°C + post cured for 1 hrs at 82°C; ASTM D638-10
Tensile Modulus 481000 psicured for 16 hrs at 21-27°C + post cured for 1 hrs at 82°C; ASTM D638-10
Compressive Strength 9950 psiPeak Stress, cured for 16 hrs at 21-27°C + post cured for 1 hrs at 82°C, 13 mm/min; ASTM D695-10
Compressive Modulus 248000 psicured for 16 hrs at 21-27°C + post cured for 1 hrs at 82°C, 13 mm/min; ASTM D695-10
Shear Strength 1900 psi
@Temperature 82.0 °C
with Scotch-Weld EW-5000; ASTM D1002-10
 3400 psi
@Temperature 71.0 °C
with Scotch-Weld EW-5000; ASTM D1002-10
 3400 psi
@Temperature 71.0 °C
No Primer; ASTM D1002-10
 3600 psi
@Temperature 71.0 °C
with Scotch-Weld EW-5000, 14 days at 71°C and 95% RH; ASTM D1002-10
 3700 psi
@Temperature -43.0 °C
with Scotch-Weld EW-5000; ASTM D1002-10
 4650 psi
@Temperature 24.0 °C
with Scotch-Weld EW-5000, 14 days at 71°C and 95% RH; ASTM D1002-10
 5000 psi
@Temperature 24.0 °C
with Scotch-Weld EW-5000; ASTM D1002-10
 5000 psi
@Temperature 24.0 °C
No Primer; ASTM D1002-10
Peel Strength 33.0 pliwith Scotch-Weld EW-5000; ASTM D3167-10
 
Processing PropertiesOriginal ValueComments
Cure Time 1.00 hour
@Temperature 82.0 °C
Full
 24.0 hour
@Temperature 24.0 °C
Full
 
Descriptive Properties
AppearanceGrayPart A
 WhitePart B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMM35420 / 170167

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.