System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Ineos ABS Triax® KU2-3154 ABS + Polyamide Blend (DAM), Injection Molding Grade
(discontinued **)
Categories:
Polymer
;
Thermoplastic
;
ABS Polymer
;
Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend
;
Nylon (Polyamide PA)
Material Notes:
Triax® KU2-3154 is mineral reinforced, easy-flowing, injection molding grade, and comes in pellets. It has reduced moisture absorption and very low warpage.
The product transitioned to the Terblend® product line.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.11
g/cc
0.0401
lb/in³
ISO 1183
Filler Content
8 %
8 %
ISO 3451-1
Water Absorption
1.3 %
1.3 %
ISO 62
Water Absorption at Saturation
3.9 %
3.9 %
ISO 62
Linear Mold Shrinkage, Flow
0.0055
cm/cm
0.0055
in/in
Test Condition: 60x60x2; 260°C / MT 80°C; 500 bar; ISO 294-4
Linear Mold Shrinkage, Transverse
0.0060
cm/cm
0.0060
in/in
Test Condition: 60x60x2; 260°C / MT 80°C; 500 bar; ISO 294-4
Melt Flow
8.5
g/10 min
@Load 5.00 kg,
Temperature 260 °C
8.5
g/10 min
@Load 11.0 lb,
Temperature 500 °F
ISO 1133
Mechanical Properties
Metric
English
Comments
Tensile Strength at Break
38.0
MPa
5510
psi
5 mm/min; ISO 527-1,-2
Tensile Strength, Yield
55.0
MPa
7980
psi
50 mm/min; ISO 527-1,-2
Elongation at Break
35 %
35 %
5 mm/min; ISO 527-1,-2
35 %
35 %
50 mm/min, Nominal; ISO 527-1,-2
Elongation at Yield
2.9 %
2.9 %
50 mm/min; ISO 527-1,-2
Tensile Modulus
2.70
GPa
392
ksi
1 mm/min; ISO 527-1,-2
Flexural Strength
75.0
MPa
10900
psi
2 mm/min, @ 3.5% strain; ISO 178
80.0
MPa
11600
psi
2 mm/min; ISO 178
Flexural Modulus
2.50
GPa
363
ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO)
5.00
kJ/m²
@Temperature -30.0 °C
2.38
ft-lb/in²
@Temperature -22.0 °F
ISO 180-1A
7.00
kJ/m²
@Temperature 23.0 °C
3.33
ft-lb/in²
@Temperature 73.4 °F
ISO 180-1A
Izod Impact, Unnotched (ISO)
60.0
kJ/m²
@Temperature -30.0 °C
28.6
ft-lb/in²
@Temperature -22.0 °F
ISO 180-1U
100
kJ/m²
@Temperature 23.0 °C
47.6
ft-lb/in²
@Temperature 73.4 °F
ISO 180-1U
Charpy Impact Unnotched
10.0
J/cm²
@Temperature -30.0 °C
47.6
ft-lb/in²
@Temperature -22.0 °F
ISO 179-1eU
15.0
J/cm²
@Temperature 23.0 °C
71.4
ft-lb/in²
@Temperature 73.4 °F
ISO 179-1eU
Charpy Impact, Notched
0.600
J/cm²
@Temperature -30.0 °C
2.86
ft-lb/in²
@Temperature -22.0 °F
ISO 179-1eA
0.800
J/cm²
@Temperature 23.0 °C
3.81
ft-lb/in²
@Temperature 73.4 °F
ISO 179-1eA
Electrical Properties
Metric
English
Comments
Volume Resistivity
1.00e+15
ohm-cm
1.00e+15
ohm-cm
IEC 60093
Surface Resistance
1.00e+15
ohm
1.00e+15
ohm
IEC 60093
Dielectric Constant
3.1
@Frequency 1e+6 Hz
3.1
@Frequency 1e+6 Hz
IEC 60250
3.4
@Frequency 100 Hz
3.4
@Frequency 100 Hz
IEC 60250
Dielectric Strength
40.0
kV/mm
@Thickness 1.00 mm
1020
kV/in
@Thickness 0.0394 in
IEC 60243-1
Dissipation Factor
0.015
@Frequency 100 Hz
0.015
@Frequency 100 Hz
IEC 60250
0.015
@Frequency 1e+6 Hz
0.015
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index
600
V
600
V
Solution A, Rating; IEC 60112
Thermal Properties
Metric
English
Comments
CTE, linear
65.0
µm/m-°C
@Temperature 23.0 - 55.0 °C
36.1
µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1,-2; Parallel to Flow
CTE, linear, Transverse to Flow
100
µm/m-°C
@Temperature 23.0 - 55.0 °C
55.6
µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1,-2
Deflection Temperature at 0.46 MPa (66 psi)
97.0
°C
207
°F
ISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi)
83.0
°C
181
°F
ISO 75-1,-2
Vicat Softening Point
105
°C
@Load 5.10 kg
221
°F
@Load 11.2 lb
50°C/hour; ISO 306
130
°C
@Load 1.02 kg
266
°F
@Load 2.25 lb
120°C/hour; ISO 306
Flammability, UL94
HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
Shrinkage, MD
0.10 %
@Temperature 80.0 °C,
Time 3600 sec
0.10 %
@Temperature 176 °F,
Time 1.00 hour
Post; Test Condition: 60x60x2; ISO 294-4
Shrinkage, TD
0.10 %
@Temperature 80.0 °C,
Time 3600 sec
0.10 %
@Temperature 176 °F,
Time 1.00 hour
Post; Test Condition: 60x60x2; ISO 294-4
Processing Properties
Metric
English
Comments
Melt Temperature
260
°C
500
°F
Injection Molding; ISO 294
Mold Temperature
80.0
°C
176
°F
Injection Molding; ISO 294
Injection Velocity
40.0
mm/sec
1.57
in/sec
Injection Molding; ISO 294
**
Materials flagged as discontinued (
) are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.
Users of our Advanced Search (registration required) may exclude discontinued materials from search results.
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Daicel CEVIAN® A1700 PA/ABS Alloy, DAM
Techmer ES Plastiblend® ABS/PA 1700
E-Polymers TEKAMID® H12TW Unreinforced Low warpage PA/ABS Alloy
Americhem Engineered Compounds ColorFast® NYA1000 Nylon/ABS Alloy
Techmer ES Plastiblend® ABS/PA 1700 B2
PINEA954 / 107225
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.