MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Accuratus MACOR Machinable Glass Ceramic
Categories: Ceramic; Glass; Glass Ceramic; Machinable Ceramic; Oxide

Material Notes: Macor is cast as a two phase glass. After casting, it is heat treated causing crystallization of one phase giving rise to its glass-like and ceramic-like characteristics.

Key Properties of MACOR: Machinable Glass Ceramic; Low thermal conductivity; Low dielectric constant; High electrical resistance; Excellent resistance to high voltage puncture; Easily machined; Hermetic with no post-machining firing required

Typical Uses of MACOR: Machinable Glass Ceramic; Electrical spacers in vacuum systems; Thermal insulators in heated or cooled assemblies; High intensity lamp reflectors; Crystal supports; Laser cavity components; Microcircuit and photonics packaging

General MACOR Machinable Glass Ceramic Information: Macor exhibits good thermal shock resistance and mechanical toughness when compared to conventional glasses with similar thermal and mechanical properties.
Macor is usable in an air atmosphere to 1000° C. In vacuum systems, where the temperature exceeds 600° C, fluorine evolution will occur manifesting itself as boron trifluoride or hydrofluoric acid.
Macor is attacked by halogen acids at elevated temperatures. It is significantly more resistant to NaOH. Alkali salts have a negligible corrosion effect.
Macor is easily machined using standard metal working tools. It is fully dense and hermetic requiring no firing after machining to develop it’s physical properties. Tolerances of less than 10 microns (.0005") are easily maintained.

Information provided by Accuratus.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.52 g/cc
Porosity 0.00 %
 
Mechanical PropertiesOriginal ValueComments
Modulus of Elasticity 66.9 GPa
Flexural Strength 94.0 MPa
Compressive Strength 345 MPa
Poissons Ratio 0.29
Fracture Toughness 1.53 MPa-m½
Shear Modulus 25.5 GPa
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+14 ohm-cm
Dielectric Constant 6.0
@Frequency 1000 Hz
Dielectric Strength 40.0 kV/mm
Dielectric Loss Index 0.0050
@Frequency 1000 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 12.6 µm/m-°C
Specific Heat Capacity 0.790 J/g-°C
Thermal Conductivity 1.50 W/m-K
Maximum Service Temperature, Air 1000 °Cno load
 
Descriptive Properties
ColorWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Corning Macor® Machinable Glass Ceramic
Borosilicate Glass
Aremco AREMCOLOX™ 502-800 Macor® Machinable Glass Ceramic, MGC
Corundum, Aluminum Oxide, Alumina, 99.9%, Al2O3
96% Silica Consolidated Reconstructed Glass

CACCUR02 / 129645

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.