MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Lubrizol STAT-RITE® E-1140 Ester-Type Static Dissipative Polymer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane, TP

Material Notes: Description: Stat-Rite® E-1140 is a static dissipative thermoplastic polyurethane (TPU) alloy. Stat-Rite E-1140 utilizes the patented Stat-Rite inherently dissipative polymer (IDP) alloy system to provide clean, permanent ESD protection. Stat-Rite alloys retain uniform static dissipation properties even when injection molded or extruded.

Features:

  • Permanently static dissipative
  • Does not require humidity
  • Ultra-clean: low off-gassing, low ionics
  • See-through clarity
  • No particulates

Applications:

  • Cleanroom soft walls, windows and doors
  • Vacuum tubing
  • Work surface mats

Available in Americas, Europe, Middle East, Africa, India and Asia

Information provided by Lubrizol.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 82ASTM D2240
Tensile Strength at Break 30.0 MPaASTM D412
Elongation at Break 670 %ASTM D412
100% Modulus 0.00510 GPa
@Strain 100 %
ASTM D412
300% Modulus 0.00800 GPa
@Strain 300 %
ASTM D412
Tear Strength 65.0 kN/mASTM D646
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 2.00e+10 ohm-cmASTM D257
Surface Resistance 1.00e+10 ohmASTM D257
Surface Resistivity per Square 1.10e+11 ohmASTM D257
Static Decay 0.90 sec12% RH (+5000 V to 50 V); FTMS-101C
 0.90 sec12% RH (-5000 V to -50 V); FTMS-101C
 
Processing PropertiesOriginal ValueComments
Drying Temperature 105 °Cdehumidifying hopper
Dry Time 2.00 - 3.00 hour
 
Descriptive Properties
ColorTransparent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lubrizol STAT-RITE® E-1150 Ether-Type Static Dissipative Polymer
Lubrizol STAT-RITE® S-1100 Static Dissipative TPU
Lubrizol STAT-RITE® S-1107 Static Dissipative TPU
Lubrizol Stat-Rite® S-250 Static Control Polypropylene
Lubrizol Stat-Rite® SIS535 Static Control System

PNOVEON068 / 55333

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.