MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
RTP Company RTP 2202 HF TFE 15 Polyetheretherketone (PEEK), Glass Fiber - PTFE Lubricated
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Glass Fiber Filled

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.53 g/ccASTM D 792
Additive Loading 15 %Primary Additive
Linear Mold Shrinkage 0.0030 - 0.0060 cm/cm
@Thickness 3.17 mm
ASTM D 955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 13500 psiASTM D 638
Elongation at Break 1.5 - 3.5 %ASTM D 638
Tensile Modulus 1000 ksiASTM D 638
Flexural Strength 22500 psiASTM D 790
Flexural Modulus 900 ksiASTM D 790
Izod Impact, Notched 1.50 ft-lb/in
@Thickness 3.17 mm
ASTM D 256
Izod Impact, Unnotched 9.50 ft-lb/in
@Thickness 3.17 mm
ASTM D 4812
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 500 °FASTM D 648
Flammability, UL94 V-0
@Thickness 1.59 mm
 
Processing PropertiesOriginal ValueComments
Melt Temperature 660 - 750 °F
Mold Temperature 325 - 425 °F
Drying Temperature 300 °F
@Time 10800 sec
Moisture Content 0.10 %
Dew Point -20.0 °F
Injection Pressure 12000 - 18000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polyetheretherketone, Glass Fiber Filled
Mitsubishi Chemical Advanced Materials Ketron™ GF30 PEEK, Extruded 30% Glass-Reinforced Polyetherether Ketone
LATI Laramid G/60 PPA, 60% Glass Fiber Reinforced
Evonik Trogamid® T-GF35 35% Glass Reinforced Amorphous Nylon
Evonik Trogamid® BX9724 40% Glass Reinforced Nylon Blend

PQZTA25049 / 159235

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.