MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
KEP Kepital® F10 Standard Grade/High Viscosity Acetal Homopolymer
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Homopolymer, Unreinforced

Material Notes: Extrusion: electrical parts, machine/mechanical parts, industrial parts, automotive parts, applications, electronic data processing parts, thick-walled

Kepital® is a registered trademark of Korea Engineering Plastics Co., Ltd. Information provided by Dayson Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.41 g/ccASTM D792
Water Absorption 0.22 %24 hrs.; ASTM D570
Linear Mold Shrinkage, Flow 0.022 cm/cmASTM D955
Melt Flow 30 g/10 min
@Load 2.16 kg,
Temperature 190 °C
Condition E; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 78ASTM D785
Tensile Strength at Break 8750 psiASTM D638
Elongation at Break 65 %
Flexural Yield Strength 12800 psiASTM D790
Flexural Modulus 372700 psiASTM D790
Izod Impact, Notched 1.30 ft-lb/in0.126 inches; ASTM D256
Tensile Impact Strength 56.0 ft-lb/in²0.0630 in; ASTM D1822
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 ohm-cmASTM D257
Surface Resistance 1.00e+16 ohmASTM D257
Dielectric Constant 3.7
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 483 V/milASTM D149
Dissipation Factor 0.0070
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 72.0 µin/in-°F
@Temperature 20.0 °C
ASTM D696
Melting Point 329 °F
Deflection Temperature at 0.46 MPa (66 psi) 316 °FUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 230 °FUnannealed; ASTM D648
Flammability, UL94 HB
@Thickness 0.800 mm
 HB
@Thickness 6.40 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Delrin Delrin® 911DP NC010 POM
Delrin Delrin® FG511DP NC010 POM
KEP Kepital® F10-52D Acetal Copolymer, UV-stabilized
Mitsubishi Iupital® F10-01, F10-02 Copolymer Acetal
Aardvark Polymers AARTEL® 1000 Rotational Molding Resin

PFORDA17 / 38801

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.