MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Michelman® Michem® Coat 40 Plus N Water resistant, gluable coating
Categories: Fluid; Polymer; Thermoplastic; Adhesives, Sealants, and Coatings

Material Notes: Michem® Coat water-based coatings are selected primarily for grease and oil resistance. Other benefits include water resistance, release, coldset gluability, hot melt gluability, recyclability, and compliance with specific food contact regulations. Michem® Coat 40 Plus N can be applied either in-line or off-line on the corrugator at the wet or dry end, via rod or blade. Usage: A water based coating designed to provide good water resistance to corrugated board. It is cold set gluable with most adhesives.

Applications (properties imparted): Food Service (water resistance), Perishables (water resistance).

Handling: Handle in accordance with good industrial hygiene and safety practice. Use personal protective equipment as required.

Information provided by Michelman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
pH 5.0 - 10
Brookfield Viscosity 200 - 800 cPSpindle #3. 60 RPM.
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 MonthDry, cool and well-ventilated place
 
Descriptive Properties
AppearanceWhite, semi-viscous liquid
EZ Cup Viscosity (sec)25 - 35Cup #3
Solids TypeSynthetic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WMICHE9892 / 287487

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.