MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Special Metals INCOTHERM® TD Nickel Alloy
Categories: Metal; Nonferrous Metal; Nickel Alloy; Superalloy; Nickel Base

Material Notes: INCOTHERM® alloy TD is recommended for thermocouple sheathing where high-temperature corrosion resistance and strength are required without the use of elements that may cause thermocouple degradation over time.

Elements such as manganese and aluminum, which can diffuse through the thermocouple insulator and contaminate the thermo-element wires leading to emf drift over time, are controlled at very low levels thus giving excellent long term performance. The composition is similar to the thermo-element wires, which further reduces the potential for the diffusion of elements between the alloys. The alloy has outstanding static and cyclic oxidation resistance at temperatures up to at least 1250°C (2282°F).

INCOTHERM alloy TD is highly resistant to oxide spalling and can be considered for applications where contamination needs to be controlled at low levels, such as in glass making and electronic component processing.

Information Provided by Special Metals Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.17 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 90.0 MPa
@Temperature 1000 °C
 280 MPa
@Temperature 800 °C
 440 MPa
@Temperature 600 °C
 560 MPa
@Temperature 400 °C
 680 MPa
@Temperature 200 °C
 800 MPa
@Temperature 20.0 °C
Tensile Strength, Yield 30.0 MPa
@Temperature 1000 °C
 170 MPa
@Temperature 800 °C
 220 MPa
@Temperature 600 °C
 290 MPa
@Temperature 400 °C
 350 MPa
@Temperature 200 °C
 400 MPa
@Temperature 20.0 °C
Elongation at Break 50 %
@Temperature 20.0 °C
 58 %
@Temperature 200 °C
 65 %
@Temperature 400 °C
 73 %
@Temperature 600 °C
 81 %
@Temperature 800 °C
 81 %
@Temperature 1000 °C
Rupture Strength 4.00 MPa
@Temperature 1200 °C,
Time 6.12e+6 sec
 5.00 MPa
@Temperature 1177 °C,
Time 9.00e+6 sec
 6.00 MPa
@Temperature 1177 °C,
Time 3.06e+6 sec
 7.00 MPa
@Temperature 1100 °C,
Time 7.92e+6 sec
 9.50 MPa
@Temperature 1100 °C,
Time 2.16e+6 sec
 10.0 MPa
@Temperature 1100 °C,
Time 504000 sec
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.000116 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 14.6 µm/m-°C
@Temperature 500 °C
 15.0 µm/m-°C
@Temperature 600 °C
 15.59 µm/m-°C
@Temperature 700 °C
 16.1 µm/m-°C
@Temperature 800 °C
 16.81 µm/m-°C
@Temperature 900 °C
 17.30 µm/m-°C
@Temperature 1000 °C
Melting Point 1380 - 1400 °C
Solidus 1380 °C
Liquidus 1400 °C
Maximum Service Temperature, Air >= 1250 °Coxidation resistance
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.01 %
Chromium, Cr 22 %
Molybdenum, Mo 3 %
Nickel, Ni 73.6 %Balance
Silicon, Si 1.4 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
MarkeTech WCu25 Tungsten Copper Alloy
Special Metals INCONEL® 690 Nickel Superalloy, Cold Drawn Tube, 0.50 inch (12.7 mm) o.d. and 0.050 inch (1.27 mm) Thickness
Eastman Tritan™ MX810 Medical Grade Copolyester
Eagle Brass 18665 MSP1, Hard
Copper, Cu; Annealed

NINDA24 / 191482

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.