MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Konson CTP-80 Masterbatch
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Composition: 80% N-(cyclohexylthio) phthalimide, 20% EPDM binder and dispersing agents

Use Characteristics: Konson® CTP-80 retards the onset of cure in NR and diene sythetic rubber without considerably extending the total curing time. It is preferably used with sulphenamide or thiazole accelerators to improve processing safety, keeping the properties of the vulcanizate unchanged. Konson® CTP-80 significantly improves the storage stability of uncured diene rubber compounds. When Konson® CTP-80 is used in the compounds, it is possible to process the rubber compounds at higher temperatures, thereby ensuring full use of machine capacity. Contact staining does not occur. Konson® CTP-80 causes only very slight discolouration in bright or white articles.

Processing Advantages: The thermoplastic, excellent compatible EPDM/EVA binder which is combined with active dispersing promoters allows much more easily and quickly incorporation and excellent dispersion in the rubber mixing. In this way, optimal activity of the effective CTP is assured.

Dosage levels: Normally 0.2 - 2.0 phr

Applications: Compounds based on synthetic diene rubber and natural rubber, which are mainly cured with thiazole and sulphenamide accelerators (e.g. in the production of tires, conveyor belts, soles, technical moulded and extruded articles.

Information provided by Konson®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.23 g/cc
Ash <= 0.40 %
Evaporation Loss <= 0.50 %
 
Thermal PropertiesOriginal ValueComments
Melting Point 85.0 °C
 
Descriptive Properties
AppearanceBeige granules
Content= 98%CTP
Sieve residue= 0.1 %63µm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PKONS030 / 256075

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.