MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Aperam AFK 502R Cold Rolled Strip
Categories: Metal; Ferrous Metal

Material Notes: AFK502R is an Iron-Cobalt soft magnetic alloy suitable for compact generators, motor and transformer laminations.

All values declared are typical values measured on rings 36x25mm of 0.34mm material thickness.

International standards: ASTM A 801, IEC404

Information provided by Aperam

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.12 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 33 - 47Hard Temper
Hardness, Vickers 400Hard Temper
Tensile Strength, Ultimate 1200 MPaHard Temper
 450 MPa
@Treatment Temp. 850 °C,
Time 10800 sec
 600 MPa
@Treatment Temp. 760 °C,
Time 7200 sec
Tensile Strength, Yield 800 MPaHard Temper
 290 MPa
@Treatment Temp. 850 °C,
Time 10800 sec
 390 MPa
@Treatment Temp. 760 °C,
Time 7200 sec
Elongation at Break 2.0 %Hard Temper
 4.0 %
@Treatment Temp. 850 °C,
Time 10800 sec
 5.0 %
@Treatment Temp. 760 °C,
Time 7200 sec
Tensile Modulus 215000 MPaYoung, Hard
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 0.000040 ohm-cm
Magnetic Coercive Force, Hc 0.90 Oe
@Treatment Temp. 850 °C,
Time 10800 sec
 1.5 Oe
@Treatment Temp. 760 °C,
Time 7200 sec
Magnetic Saturation Flux Density, Bmax 24000 GaussSaturation Induction
Curie Temperature 900 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 10.0 µm/m-°C
@Temperature 0.000 - 100 °C
 
Component Elements PropertiesOriginal ValueComments
Cobalt, Co 49 %
Iron, Fe 49 %
Vanadium, V 2.0 %
 
Descriptive Properties
Magnetic DC, B>205000 @ 10Oe2h at 760°C
 >210000 @ 10Oe3h at 850°C
 >215000 @ 25Oe2h at 760°C
 >215000 @ 25Oe3h at 850°C
 >22500 @ 50Oe2h at 760°C
 >22500 @ 50Oe3h at 850°C
 >22800 @ 100Oe2h at 760°C
 >22800 @ 100Oe3h at 850°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aperam Supera 40 Cold Rolled Strip
Aperam Supermimphy® L Cold Rolled Strip
Aperam Permimphy SP Cold Rolled Strip
Ferrite 1, Sintered Iron-Barium Oxide Hard Magnetic Material
FloMet Fe-3% Si Soft Magnetic Alloy

NPERA003 / 194792

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.