System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Phillips Sumika Marlex® AGX-230 Polypropylene Impact Copolymer
(discontinued **)
Categories:
Polymer
;
Thermoplastic
;
Polypropylene (PP)
;
Polypropylene Copolymer
Material Notes:
Applications:
Durables
Housewares
Consumer products
Information provided by Chevron Phillips.
Phillips Sumika Polypropylene Company has been shut down, as announced in 2011. This product had been discontinued prior to the shutdown announcement.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
0.900
g/cc
@Thickness 3.17 mm
injection molded specimen; ASTM D1505
Melt Flow
20
g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
Mechanical Properties
Original Value
Comments
Hardness, Rockwell R
85
@Thickness 3.17 mm
injection molded sample; ASTM D785
Tensile Strength, Yield
23.0
MPa
2 in/min, 1/8" thick injection molded, type 1 specimen; ASTM D638
Flexural Modulus
1.10
GPa
1/8" thick injection molded specimen, 0.5 in/min, Tangent method; ASTM D790
Izod Impact, Notched
35.0
J/m
@Thickness 3.17 mm,
Temperature -30.0 °C
injection-molded specimen; ASTM D256
55.0
J/m
@Thickness 3.17 mm,
Temperature 0.000 °C
injection molded specimen; ASTM D256
110
J/m
@Thickness 3.17 mm,
Temperature 23.0 °C
injection molded specimen; ASTM D256
Falling Dart Impact
27.0
J
@Thickness 3.17 mm,
Temperature -30.0 °C
0.5" tup, 150"/sec, injection molded specimen; ASTM D3763
Thermal Properties
Original Value
Comments
Deflection Temperature at 0.46 MPa (66 psi)
80.0
°C
@Thickness 3.17 mm
injection molded specimen; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi)
50.0
°C
@Thickness 3.17 mm
injection molded specimen; ASTM D648
**
Materials flagged as discontinued (
) are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.
Users of our Advanced Search (registration required) may exclude discontinued materials from search results.
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Phillips Sumika Marlex® AGN-200 Polypropylene Impact Copolymer
Phillips Sumika Marlex® AGX-020-01 Polypropylene Impact Copolymer
ExxonMobil PP7011L1 Polypropylene Impact Copolymer
ExxonMobil PP4031E2 Polypropylene Impact Copolymer
Phillips 66 COPYLENE® CM005 Polypropylene Impact Copolymer
PCHEVD056 / 20654
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.