MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ascend Performance Materials Vydyne® 88XD Nylon 66, General Purpose  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Unreinforced

Material Notes:

Information provided by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.14 g/ccISO 1183
Water Absorption 1.4 %
@Time 86400 sec
ISO 62
Moisture Absorption at Equilibrium 2.8 %50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.018 cm/cm
@Thickness 2.00 mm
ISO 294-4
Linear Mold Shrinkage, Transverse 0.018 cm/cm
@Thickness 2.00 mm
ISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 40.0 MPaConditioned; ISO 527-2
 50.0 MPaDry; ISO 527-2
Tensile Strength, Yield 60.0 MPaConditioned; ISO 527-2
 86.0 MPaDry; ISO 527-2
Elongation at Break 27 %Dry; ISO 527-2
 >= 50 %Conditioned; ISO 527-2
Elongation at Yield 5.0 %Dry; ISO 527-2
 10 %Conditioned; ISO 527-2
Tensile Modulus 1800 MPaConditioned; ISO 527-2
 3400 MPaDry; ISO 527-2
Flexural Strength 30.0 MPaConditioned; ISO 178
 90.0 MPaDry; ISO 178
Flexural Modulus 980 MPaConditioned; ISO 178
 2900 MPaDry; ISO 178
Poissons Ratio 0.40Dry; ISO 527-2
Izod Impact, Notched (ISO) 5.00 kJ/m²
@Temperature -30.0 °C
Dry; ISO 180
 5.00 kJ/m²
@Temperature -30.0 °C
Conditioned; ISO 180
 6.00 kJ/m²
@Temperature 23.0 °C
Dry; ISO 180
 30.0 kJ/m²
@Temperature 23.0 °C
Conditioned; ISO 180
Charpy Impact Unnotched NB
@Temperature -30.0 °C
Dry; ISO 179/1eU
 NB
@Temperature -30.0 °C
Conditioned; ISO 179/1eU
 NB
@Temperature 23.0 °C
Dry; ISO 179/1eU
 NB
@Temperature 23.0 °C
Conditioned; ISO 179/1eU
Charpy Impact, Notched 5.00 kJ/m²
@Temperature -30.0 °C
Dry; ISO 179/1eA
 5.00 kJ/m²
@Temperature -30.0 °C
Conditioned; ISO 179/1eA
 6.00 kJ/m²
@Temperature 23.0 °C
Dry; ISO 179/1eA
 30.0 kJ/m²
@Temperature 23.0 °C
Conditioned; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 26.0 kV/mm
@Thickness 1.00 mm
IEC 60243
Arc Resistance 120 - 180 sec
@Thickness 3.00 mm
PLC 5; ASTM D495
Comparative Tracking Index 600 V
@Thickness 3.00 mm
IEC 60112
Hot Wire Ignition, HWI 7.0 - 15 sec
@Thickness 0.750 mm
PLC 4; UL 746
 15 - 30 sec
@Thickness 1.50 mm
PLC 3; UL 746
 15 - 30 sec
@Thickness 3.00 mm
PLC 3; UL 746
High Amp Arc Ignition, HAI >= 120 arcs
@Thickness 0.750 mm
PLC 0; UL 746
 >= 120 arcs
@Thickness 1.50 mm
PLC 0; UL 746
 >= 120 arcs
@Thickness 3.00 mm
PLC 0; UL 746
High Voltage Arc-Tracking Rate, HVTR 0.000 - 10.0 mm/minPLC 0; UL 746
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 100 µm/m-°C
@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 100 µm/m-°C
@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
ISO 11359-2
Melting Point 253 °CISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 183 °CISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 62.0 °CISO 75-2/A
UL RTI, Electrical 130 °CUL 746
 130 °C
@Thickness 0.750 mm
UL 746
 130 °C
@Thickness 1.50 mm
UL 746
 130 °C
@Thickness 3.00 mm
UL 746
UL RTI, Mechanical with Impact 75.0 °C
@Thickness 0.400 mm
UL 746
 75.0 °C
@Thickness 0.750 mm
UL 746
 75.0 °C
@Thickness 1.50 mm
UL 746
 75.0 °C
@Thickness 3.00 mm
UL 746
UL RTI, Mechanical without Impact 75.0 °C
@Thickness 0.400 mm
UL 746
 85.0 °C
@Thickness 0.750 mm
UL 746
 85.0 °C
@Thickness 1.50 mm
UL 746
 85.0 °C
@Thickness 3.00 mm
UL 746
Flammability, UL94 V-2
@Thickness 0.400 mm
 V-2
@Thickness 0.750 mm
 V-2
@Thickness 1.50 mm
 V-2
@Thickness 3.00 mm
Oxygen Index 28 %ISO 4589-1/-2
Glow Wire Ignition Temperature 700 °C
@Thickness 0.750 mm
IEC 60695-2-13
 700 °C
@Thickness 1.50 mm
IEC 60695-2-13
 700 °C
@Thickness 3.00 mm
IEC 60695-2-13
Glow Wire Flammability Index 800 °C
@Thickness 0.750 mm
IEC 60695-2-12
 800 °C
@Thickness 1.50 mm
IEC 60695-2-12
 930 °C
@Thickness 3.00 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 250 - 270 °CInjection Molding
Middle Barrel Temperature 260 - 275 °CInjection Molding
Front Barrel Temperature 270 - 280 °CInjection Molding
Nozzle Temperature 270 - 290 °CInjection Molding
Melt Temperature 275 - 290 °CInjection Molding
Mold Temperature 65.0 - 95.0 °CInjection Molding
Drying Temperature <= 70.0 °C
@Time 3600 - 10800 sec
Injection Molding
 
Compliance PropertiesOriginal ValueComments
European Food 1935/2004 Yes
FDA Yes21CFR 177.1500
 
Descriptive Properties
Agency RatingsEU 10/2011
 EU 2023/2006
 FED L-P-410A
FeaturesFast Molding Cycle
 General Purpose
 Good Mold Release
 Good Stiffness
 High Rigidity
 Lubricated
 Nucleated
Suggested Max Regrind (%)25
UsesBearings
 Cams
 Connectors
 Fasteners
 General Purpose
 Housings
 Industrial Applications

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Honeywell ACCUFLO® T27 2527 Organic Polymer
Asahi Kasei Leona™ 14025 Polyamide 66, Heat Stabilized
Asahi Kasei Leona™ 13G50 Polyamide 66, GF Reinforced
Asahi Kasei Leona™ 13005 Polyamide 66, General Purpose
Arkema Orgalloy® RS 6630 BLACK Polyamide 6.6 Alloy 30% Glass Fiber reinforced

PZASCE9752 / 220855

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.