MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Harris Acoustic Sensors EC-97 Lead Titanate Piezoelectric
Categories: Ceramic; Oxide; Titanium Oxide; Piezoelectric

Material Notes: Lead titanate niobate features the highest mode cancellation (reduced side load sensitivity) of all the solid solution piezoelectric materials - many times higher than lead zirconate titanates. Good "g" and excellent mode cancellation provide a valuable material for non-destructive testing, accelerometers, and hydrophones.

Data provided by Harris Acoustic Sensors. Harris Acoustic Sensors has acquired EDO Ceramics. This grade is available from Harris.

Key Words: PbTiO3
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 12.8 g/cc0.462 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Modulus of Elasticity 128 GPa18600 ksiYoung's Modulus
 
Electrical PropertiesMetricEnglishComments
Curie Temperature 240 °C464 °F
Dielectric Constant 270
@Frequency 1000 Hz
270
@Frequency 1000 Hz
Dissipation Factor 0.0090
@Frequency 1000 Hz
0.0090
@Frequency 1000 Hz
low field
Piezoelectric Longitudinal Coupling Factor, k33 0.530.53
Piezoelectric Transverse Voltage Coefficient, d31, 10^-12 m/V -3.00-3.00strain/field at constant stress
Piezoelectric Shear Charge Coefficient, d15, 10^-12 m/V 6767strain/field at constant stress
Piezoelectric Longitudinal Voltage Coefficient, g33, 10^-3 V-m/N 3232field/stress at constant charge density
Piezoelectric Planar Coupling Factor, kp 0.0100.010
Piezoelectric Mechanical Q 950950Thin Disk
Piezoelectric Shear Coupling Factor, k15 0.350.35
Piezoelectric Longitudinal Charge Coefficient, d33, 10^-12 m/V 6868strain/field at constant stress
Piezoelectric Transverse Voltage Coefficient, g31, 10^-3 V-m/N -1.70-1.70field/stress at constant charge density
Piezoelectric Shear Voltage Coefficient, g15, 10^-3 V-m/N 33.533.5field/stress at constant charge density
Piezoelectric Transverse Coupling Factor, k31 0.0100.010

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Harris Acoustic Sensors EC-76 Lead Zirconium Titanate Piezoelectric
Harris Acoustic Sensors EC-70 Lead Zirconium Titanate Piezoelectric
Harris Acoustic Sensors EC-63 Lead Zirconium Titanate Piezoelectric
Indium Corp. Indalloy® 97 Pb-Sn-Bi Solder Alloy
Harris Acoustic Sensors K-40 Dielectric

CEDO12 / 797

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.