MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Overview of materials for Tungsten Alloy
Categories: Metal; Nonferrous Metal; Refractory Metal; Tungsten Alloy

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Tungsten Alloy". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Eagle Alloys Corporation is a leading supplier of quality metals and alloys. Our staff prides itself on working fast, efficiently and courteously to get you the information you need. Call (800) 237-9012 or visit www.EagleAlloys.com.

Elmet Technologies is a 100% US owned and operated, fully integrated manufacturer of Molybdenum, Tungsten and related alloys such as TZM, WHA & MoLa. At our 220,000 sqr/ft plant in Lewiston, Maine, Elmet manufactures W & Mo pure powders plus rod, wire, plate, sheet & foil in additional to offering fabrication and machining services. ITAR, ISO and AS9100 registered. www.elmettechnologies.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 2.74 - 19.7 g/ccAverage value: 15.4 g/cc Grade Count:350
Particle Size 0.0350 - 325 µmAverage value: 30.0 µm Grade Count:16
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 160 - 2550Average value: 925 Grade Count:11
Hardness, Rockwell A 66.0 - 94.3Average value: 88.0 Grade Count:58
Hardness, Rockwell B 32.0 - 110Average value: 85.1 Grade Count:101
Hardness, Rockwell C 24.0 - 63.0Average value: 34.8 Grade Count:98
Hardness, Vickers 200 - 2050Average value: 975 Grade Count:92
Tensile Strength, Ultimate 350 - 4900 MPaAverage value: 865 MPa Grade Count:147
Tensile Strength, Yield 450 - 1640 MPaAverage value: 668 MPa Grade Count:102
Elongation at Break 0.000 - 30.0 %Average value: 8.47 % Grade Count:110
Modulus of Elasticity 220 - 430 GPaAverage value: 340 GPa Grade Count:84
Flexural Yield Strength 610 - 4700 MPaAverage value: 2960 MPa Grade Count:42
Compressive Yield Strength 603 - 8400 MPaAverage value: 4630 MPa Grade Count:51
Poissons Ratio 0.200 - 0.320Average value: 0.270 Grade Count:11
Fatigue Strength 276 - 465 MPaAverage value: 366 MPa Grade Count:8
Fracture Toughness 7.00 - 19.0 MPa-m½Average value: 12.5 MPa-m½ Grade Count:14
Shear Modulus 125 - 160 GPaAverage value: 150 GPa Grade Count:11
Charpy Impact 4.70 - 9.50 JAverage value: 6.60 J Grade Count:8
Charpy Impact, Unnotched 12.2 - 203 JAverage value: 71.1 J Grade Count:8
Charpy Impact, Notched 30.0 - 170 J/cm²Average value: 97.5 J/cm² Grade Count:6
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000246 - 0.0000290 ohm-cmAverage value: 0.00000701 ohm-cm Grade Count:191
Magnetic Permeability 1.05Average value: 1.05 Grade Count:24
 
Thermal PropertiesOriginal ValueComments
CTE, linear 4.40 - 12.2 µm/m-°CAverage value: 6.22 µm/m-°C Grade Count:94
Specific Heat Capacity 0.132 - 0.251 J/g-°CAverage value: 0.172 J/g-°C Grade Count:24
Thermal Conductivity 18.0 - 330 W/m-KAverage value: 155 W/m-K Grade Count:149
Melting Point 980 - 3420 °CAverage value: 2110 °C Grade Count:98
Solidus 980 - 1430 °CAverage value: 1070 °C Grade Count:67
Liquidus 1230 - 3410 °CAverage value: 3350 °C Grade Count:49
Boiling Point 5560 - 5900 °CAverage value: 5800 °C Grade Count:10
Maximum Service Temperature, Air 600 - 2760 °CAverage value: 2140 °C Grade Count:7
Minimum Service Temperature, Air 0.000 °CAverage value: 0.000 °C Grade Count:5
 
Processing PropertiesOriginal ValueComments
Recrystallization Temperature 1450 - 2600 °CAverage value: 1960 °C Grade Count:7
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 0.00150 - 0.00350 %Average value: 0.00231 % Grade Count:16
Boron, B 0.400 - 5.00 %Average value: 1.98 % Grade Count:10
Calcium, Ca 0.00300 %Average value: 0.00300 % Grade Count:3
Carbon, C 0.00300 - 6.50 %Average value: 2.21 % Grade Count:30
Chromium, Cr 0.00200 - 25.0 %Average value: 4.14 % Grade Count:31
Cobalt, Co 0.100 - 36.3 %Average value: 9.93 % Grade Count:52
Copper, Cu 0.00100 - 58.0 %Average value: 21.5 % Grade Count:123
Fe + Ni 1.50 - 10.0 %Average value: 5.30 % Grade Count:5
Iron, Fe 0.00300 - 13.5 %Average value: 1.84 % Grade Count:75
Lead, Pb 0.000500 - 0.00200 %Average value: 0.00163 % Grade Count:4
Magnesium, Mg 0.00200 %Average value: 0.00200 % Grade Count:3
Manganese, Mn 0.00200 %Average value: 0.00200 % Grade Count:3
Molybdenum, Mo 0.00500 - 50.0 %Average value: 4.18 % Grade Count:17
Ni, Fe, Mo 7.00 - 10.0 %Average value: 7.60 % Grade Count:5
Nickel, Ni 0.00200 - 56.0 %Average value: 8.25 % Grade Count:98
Oxygen, O 0.00200 - 0.0800 %Average value: 0.0210 % Grade Count:12
Potassium, K 0.000500 - 0.0100 %Average value: 0.00576 % Grade Count:19
Rhenium, Re 1.50 - 26.0 %Average value: 14.6 % Grade Count:12
Silicon, Si 0.00100 - 3.10 %Average value: 0.742 % Grade Count:28
Silver, Ag 10.0 - 58.0 %Average value: 37.7 % Grade Count:48
Sodium, Na 0.00200 %Average value: 0.00200 % Grade Count:11
Thorium, Th 1.00 - 4.00 %Average value: 2.06 % Grade Count:8
Tin, Sn 0.00200 %Average value: 0.00200 % Grade Count:3
Titanium, Ti 0.00200 - 5.00 %Average value: 1.25 % Grade Count:4
Tungsten, W 29.5 - 100 %Average value: 82.9 % Grade Count:293
WC 42.0 - 97.0 %Average value: 75.8 % Grade Count:70

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Nickel Alloy
Overview of materials for Refractory Metal
Overview of materials for Stainless Steel
Overview of materials for Molybdenum Alloy
Overview of materials for Cobalt Alloy

M01074 / 81679

Metalmen Sales

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.