MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Glyptal C1800 Enamel
Categories: Polymer; Thermoset; Epoxy; Epoxy Cure Resin

Material Notes: GLYPTAL C-1800 is designed as a quick-dry, high viscosity gasket seal. The C-1800 red enamel is an excellent protective coating suitable for almost all types of equipment where oil, moisture, and acid resistance as well as good weatherability are desired. It has superior thermal resistance. C-1800 is also very useful in a variety of pipe-thread compound, gasket adhesive, vacuum system sealer, etc.

Information provided by Glyptal Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 12.1 lb/gal
Solids Content 51 - 55 %Volume
Fineness >= 3.0Hegman
Viscosity 4000 - 4400 cP
 
Optical PropertiesOriginal ValueComments
Gloss >= 15 %60°
 
Processing PropertiesOriginal ValueComments
Cure Time 0.333 - 0.500 hourTackfree
 
Descriptive Properties
ColorRed Iron Oxide
Coverage851 ft²/gal1 mil dry film thickness
MethodDip or Brush

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PGLYPT924 / 209763

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.