MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Bayflex® 970 Polyether-based Polyurethane System, Density 34 pcf
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Characterization: Bayflex 970 is a fully compounded polyether-based polyurethane system consisting of two liquid components which can be water-blown.

Properties / Applications: Bayflex 970 is a fully compounded polyether-based polyurethane system consisting of two liquid components which can be water-blown. Component A is a modified diphenylmethane diisocyanate (MDI) prepolymer, and Component B is a polyether polyol system. The Bayflex 970 system is used in the manufacture of microcellular polyurethane shoe soles. Soles prepared from these components combine light weight, comfort, and durability. Processibility and dynamic flexural properties are excellent over a wide range of densities. The combination of excellent physical properties and ease of processing has made the Bayflex 970 system a prime soling material for sandals, fashion and casual shoes. As with any product, use of the Bayflex 970 system in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.500 g/cc0.500 g/ccMolded
 1.04 g/cc1.04 g/ccPolyol (Component B)
 1.19 g/cc1.19 g/ccIsocyanate (Component A)
Viscosity 400 cP400 cPIsocyanate (Component A)
 1100 cP1100 cPPolyol (Component B)
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5252ASTM D2240
Tensile Strength at Break 3.10 MPa450 psiASTM D412
Elongation at Break 400 %400 %ASTM D412
Tear Strength 4.38 kN/m25.0 pliBlack
 14.0 kN/m80.0 pliDie C; ASTM D1004
Taber Abrasion, mg/1000 Cycles 70
@Load 1.00 kg
70
@Load 2.20 lb
H-18; ASTM D4060
 
Thermal PropertiesMetricEnglishComments
Flash Point >= 93.0 °C>= 199 °FIsocyanate (Component A)
 138 °C280 °FPolyol (Component B)
 
Processing PropertiesMetricEnglishComments
Mold Temperature 49.0 °C120 °F
Moisture Content <= 0.45 %<= 0.45 %Polyol (Component B)
 
Descriptive Properties
AppearanceLight yellow to yellow liquidIsocyanate (Component A)
 White liquidPolyol (Component B)
Content18.9%NCO, Isocyanate (Component A)
Hydroxyl numberPolyol (Component B)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lubrizol Advanced Materials Pearlthane® Clear 15N70 Polyether based TPU
Covestro Texin® 5286 Thermoplastic Polyurethane, Polyether-based, Medical
Covestro Texin® 5290 Thermoplastic Polyurethane, Polyether-based, Medical
Covestro Texin® DP7-3006 Thermoplastic Polyurethane, Polyether-based, Aliphatic
SK Chemicals SKYTHANE® R180A Polyether Based Thermoplastic Polyurethane Elastomer

PCOVEST0132 / 201915

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.