MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
A. Schulman BMC 610 Mineral filled, glass-fiber-reinforced polyester compound
Categories: Polymer; Thermoset; Polyester, TS; Thermoset Polyester Glass and Mineral Filled BMC

Material Notes: BMC 610 molding compound is a mineral filled, glass­ fiber­ reinforced polyester compound suitable for compression, transfer and stuffer injection molding It is set a part form other medium impact electrical grade materials by its very high arc resistance and outstanding flame resistance in thin sections. Typical applications include transformer bobbins, terminal boards, arc chutes and contactors. BMC 610 molding compound is produced in extruded form in a range on industrial colors. It is available in logs up to 12 inches in length or as precut slugs, of specific weight, in diameters 1” to 2 ½” . Within this range, smaller diameters are supplied as multiple extrusion and weight tolerances are plus or minus 5 %, up to a maximum of plus or minus 15 grams.

Information provided by Bulk Molding Compounds

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.88 - 1.92 g/ccmolded
Water Absorption 0.10 %
@Temperature 23.0 °C,
Time 86400 sec
Linear Mold Shrinkage 0.0025 - 0.0045 in/in
 
Mechanical PropertiesOriginal ValueComments
Hardness, Barcol 30 - 40
Tensile Strength at Break 6000 - 8000 psi
Flexural Yield Strength 14.0 - 18.0 ksi
Compressive Strength 24000 - 28000 psi
Izod Impact, Unnotched 2.00 - 4.00 ft-lb/in
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 5.5
@Frequency 60 Hz
Dielectric Strength 360 V/mil
Dissipation Factor 0.015
@Frequency 60 Hz
Arc Resistance <= 210 sec
Track Resistance <= 54000 sec2.5 kv, Inclined plane
Comparative Tracking Index <= 600 V
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) >= 500 °F
Flammability, UL94 V-0
@Thickness 3.00 mm
 V-0
@Thickness 1.50 mm
 V-0
@Thickness 1.09 mm
 5VB
@Thickness 1.70 mm
 
Processing PropertiesOriginal ValueComments
Mold Temperature 280 - 330 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
A. Schulman BMC 605 Mineral Filled, Glass Fiber Reinforced Polyester Compound
A. Schulman BMC 610 Mineral Filled, Glass Reinforced Polyester Compound
A. Schulman BMC T44 High Strength Mineral Filled Molding Compound
A. Schulman BMC 300 Mineral Filled, Glass Reinforced Polyester
A. Schulman BMC 610 - SP Mineral Filled, Glass Reinforced Polyester Compound, with UV Stabilizer

PBMC962 / 135934

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.