MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LG Chemical LUPOY GP5206F PC/ABS+GF20%, Flame Retardance
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Glass Fiber Filled; Polycarbonate (PC)

Material Notes: Description: Injection Molding, PC/ABS+GF20%, Flame Retardance, General Purpose

Application: IT/OA (Housing)

CAS: 103598-77-2, 9003-56-9, 68928-70-1, 1309-64-4 and 65997-17-3

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.35 g/ccASTM D792
Maximum Moisture Content 0.020Injection Molding
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cm
@Thickness 3.20 mm
ASTM D955
Melt Flow 3.0 g/10 min
@Load 2.16 kg,
Temperature 250 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 117ASTM D785
Tensile Strength, Yield 950 kg(f)/cm²
@Thickness 3.20 mm
50mm/min; ASTM D638
Elongation at Break 4.0 %
@Thickness 3.20 mm
50mm/min; ASTM D638
Flexural Yield Strength 1400 kg(f)/cm²
@Thickness 3.20 mm
10mm/min; ASTM D790
Flexural Modulus 58000 kg(f)/cm²
@Thickness 3.20 mm
10mm/min; ASTM D790
Izod Impact, Notched 7.00 kg-cm/cm
@Thickness 3.20 mm,
Temperature 23.0 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 120 °C
@Thickness 6.40 mm
Unannealed; ASTM D648
UL RTI, Electrical 60.0 °C
@Thickness >=1.70 mm
UL RTI, Mechanical with Impact 60.0 °C
@Thickness >=1.70 mm
UL RTI, Mechanical without Impact 60.0 °C
@Thickness >=1.70 mm
Flammability, UL94 V-0
@Thickness >=1.70 mm
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 220 - 240 °CInjection Molding
Middle Barrel Temperature 235 - 255 °CInjection Molding
Front Barrel Temperature 250 - 265 °CInjection Molding
Nozzle Temperature 250 - 265 °CInjection Molding
Melt Temperature 235 - 265 °CInjection Molding
Mold Temperature 50.0 - 80.0 °CInjection Molding
Drying Temperature 75.0 - 85.0 °CInjection Molding
Dry Time 3.00 - 5.00 hourInjection Molding
Back Pressure 0.00200 - 0.00600 MPaInjection Molding
Screw Speed 40 - 70 rpmInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LG Chemical LUPOY GN5201F PC/ABS+GF20%, Halogen Free Flame Retardant
Overview of materials for Polycarbonate/ABS Alloy, Glass Fiber Filled
LG Chemical LUPOY GP-2401F General Purpose Modified PC, 40% Glass Fiber Reinforced, Flame Retardant
LG Chemical LUPOY GP5106F PC/ABS+GF10%, Flame Retardance
Avient Edgetek® CY-20GF/000 UV FR V0 PC/ABS Blend, Glass Filled

PLAY602 / 148612

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.