MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Covestro Desmopan® 385 Thermoplastic Polyurethane
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyester Grade

Material Notes: Desmopan 385 is a TPU on the basis of a standard ester.

Applications: Screen sections, films, hoses, seals, technical automotive parts.

Information provided by Bayer.

As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.

Key Words: TPUR
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 85DIN 53505
Elongation at Break >= 50 %Nominal
Compression Set 55 %
@Temperature 70.0 °C
24 hr
 30 %
@Temperature 22.0 °C,
Time 252000 sec
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 8.00e+11 ohm-cm
Surface Resistance 5.00e+11 ohm
Dielectric Constant 5.6
@Frequency 1e+6 Hz
 6.5
@Frequency 100 Hz
Dielectric Strength 17.5 kV/mm
Dissipation Factor 0.029
@Frequency 100 Hz
 0.060
@Frequency 1e+6 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 150 µm/m-°C
@Temperature 20.0 °C
Flammability, UL94 V-2
@Thickness 1.60 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Desmopan® 385 S Polyurethane
Covestro Desmopan® 385 E Polyurethane
Covestro Desmopan® 392 Thermoplastic Polyurethane
Covestro Desmopan® 588 Thermoplastic Polyurethane
Covestro Desmopan® 487 Thermoplastic Polyurethane

PBA105 / 26699

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.