Product Description: DuraStar™ Copolyester MN630 does not contain a mold release. It has excellent appearance and is nearly water-clear. Its most outstanding feature is its high flow characteristic, with the ability to fill intricate tooling. It is easy to process with minimal drying time and has good toughness and chemical resistance. Application/Uses: - Blood Contact
- Drug Delivery
- IV Components
- Medical
- Surgical Instruments
Key Attributes:- Chemical resistance to most medical solvents including lipids and IPA
- Ease of processing
- Gamma and E-beam color stability
|