MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

NuSil MED-6350 Gel - Restricted Medical Use
Categories: Polymer; Thermoset; Silicone

Material Notes: Description: A silicone gel is an unreinforced, loosely crosslinked network of polymers. Due to the lack of reinforcing filler, gels tend to be low in viscosity in the uncured state, allowing flexibility for various processing techniques. Not only can the crosslink density of the silicone polymers be designed to yield a very firm or soft gel, but the work time and cure profile can also be modified. Accordingly, gels can be used in a variety of applications, including sheeting and encapsulating sensors or electronic devices. Additionally, NuSil’s restricted tacky gels can be used as temporary adhesives.

Important Properties: Silicone gels have a long history of biocompatibility. The following list highlights the properties that make silicone gel systems valuable in the healthcare field:

  • Solvent-free
  • Modifiable tack and penetration
  • Varying viscosities
  • Adjustable cure profiles
  • Non-allergenic
  • Superior breathability
Comments: Low Penetration, Medium Tack Gel

Cure System: Platinum

Information provided by NuSil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 22000 cP22000 cP
 
Mechanical PropertiesMetricEnglishComments
Penetration 1.7
@Time 15.0 sec
1.7
@Time 0.00417 hour
[mm], 19.5g shaft weight, 6.35 in foot diameter
 
Processing PropertiesMetricEnglishComments
Cure Time 30.0 min
@Temperature 100 °C
0.500 hour
@Temperature 212 °F
Working Life 120 min
@Temperature 25.0 °C
120 min
@Temperature 77.0 °F
 
Descriptive Properties
Mix Ratio1:1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow Silastic® MEDICAL ADHESIVE SILICONE, TYPE A
NuSil MED-6345 Gel - Restricted Medical Use
NuSil MED3-4213 Silicone, Two part Adhesive - Unrestricted Medical Use
NuSil MED-4750 Two-Part Standard High Consistency Elastomers - Unrestricted Medical Use
Dow 3-4222 DIELECTRIC FIRM GEL KIT

PNUSIL466 / 142190

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.