System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Garlock 2900 Compressed Aramid Fiber Gasketing, Nitrile Binder
Categories:
Polymer
;
Thermoset
;
Rubber or Thermoset Elastomer (TSE)
Material Notes:
Aramid fibers with a nitrile binder.
Ideal for utility services
Excellent sealability
Improved thermal stability
Good for general service
Media: Water, aliphatic hydrocarbons, oils, gasoline
Information provided by Garlock Rubber Technologies
Key Words:
butadiene acrylonitrile
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
105
lb/ft³
Mechanical Properties
Original Value
Comments
Tensile Strength
1500
psi
across grain; ASTM F152
Electrical Properties
Original Value
Comments
Dielectric Strength
254
V/mil
@Temperature 121 °C,
Time 10800 sec
0.125 in. thickness; ASTM D149
>=
342
V/mil
@Temperature 121 °C,
Time 10800 sec
0.0625 in. thickness; ASTM D149
26.0
V/mil
@Thickness 1.59 mm
100% RH for 96 hours; ASTM D149
28.0
V/mil
@Thickness 3.17 mm
100% RH for 96 hours; ASTM D149
Thermal Properties
Original Value
Comments
Maximum Service Temperature, Air
700
°F
400
°F
@Pressure 6.89 MPa
Continuous
Minimum Service Temperature, Air
-40.0
°F
Descriptive Properties
Color
Black
Compressibility, %
7-17
ASTM F36
Creep Relaxation, %
25
ASTM F38
Sealability ASTM F37B, ml/hr
0.25
ASTM Fuel A
1
Nitrogen
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Nitrile Rubber (NBR, Acrylonitrile-Butadiene Rubber)
Garlock 361 Nitrile Sheet Rubber
Garlock 362 Nitrile Sheet Rubber
Garlock 5360 Nitrile Sheet Rubber
DuBois Aluminum Casting Salt AC Aluminum Casting Salt
PGARL801 / 157481
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.