MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Evonik VESTANAT® HT 2500 L Polyisocyanate
Categories: Polymer

Material Notes: VESTANAT HT 2500 is an aliphatic polyisocyanate based on hexamethylene diisocyanate. It contains isocyanurate groups and has a functionality between 3 and 4.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.13 g/cc
@Temperature 23.0 °C
0.0408 lb/in³
@Temperature 73.4 °F
DIN EN ISO 2811
Viscosity 400 - 700 cP
@Temperature 25.0 °C
400 - 700 cP
@Temperature 77.0 °F
DIN EN ISO 3219
 
Thermal PropertiesMetricEnglishComments
Flash Point 50.0 °C122 °Fclosed cup; DIN 53 213
 
Descriptive Properties
Hazen Color Index, max40DIN ISO 6271
NCO content (% wt)19.3-19.9EN ISO 11 909
Nonvolatile matter (%)89-91EN ISO 3251

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHUMB400 / 81402

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.