MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Precision Polymer Engineering S50K Silicone Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Silicone

Material Notes: Silicone Rubber, 45-55 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. Formulated using only those ingredients determined by the United States Federal Food and Drug Administration (FDA) to be in accordance with Code of Federal Regulations, Title 21 (CFR21), Section 177.2600. Formulated to BS2494 Type ‘W’ and Water Research Council (WRC) tested in accordance with BS6920 ‘Items which have passed full tests of effects on water quality’ (for use in potable water applications). ASTM & ISO designation = VMQ. WRC Approval No. 9910521.

Applications: Cold and hot water, plus low pressure steam, up to +110°C.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5050°IRHD; ASTM D1415
 45 - 5545 - 55°IRHD, ±5 change after 168 hours @ 70°C; ASTM D1415
Tensile Strength, Yield 9.00 MPa1310 psiASTM D412
 7.20 - 10.8 MPa1040 - 1570 psi±20% change after 168 hours @ 70°C; ASTM D412
Elongation at Break 375 %375 %ASTM D412
 262.5 - 487.5 %262.5 - 487.5 %±30% change after 168 hours @ 70°C; ASTM D412
Compression Set 12 %
@Temperature 23.0 °C,
Time 252000 sec
12 %
@Temperature 73.4 °F,
Time 70.0 hour
ASTM D395
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 250 °C482 °F
Minimum Service Temperature, Air -60.0 °C-76.0 °F
 -60.0 °C-76.0 °FNon-brittle after 3 minutes
Flash Point >= 300 °C>= 572 °F
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Precision Polymer Engineering S60G Silicone Rubber
Precision Polymer Engineering S60X Silicone Rubber
Precision Polymer Engineering S60S Silicone Rubber
Precision Polymer Engineering S60A Silicone Rubber
Precision Polymer Engineering S50R Silicone Rubber

PPRECI235 / 57959

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.