MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow DOWLEX™ 2553 Linear Low Density Polyethylene, Narrow MW Distribution
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE)

Material Notes: DOWLEX® 2553 Polyethylene resin is a narrow molecular weight distribution copolymer designed to offer good environmental stress crack resistance and impact strength with excellent stiffness for housewares, containers, and large toys. It has good processability over a wide range of extrusion coating conditions. This material complies with U.S. FDA Regulation 21 CFR 177.1520 (c) 3.2 (a) for food packaging applications. The regulation should be consulted for complete details.

Data provided by Dow Chemical.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.935 g/cc0.0338 lb/in³
Viscosity  37000 cP
@Shear Rate 5000 1/s,
Temperature 190 °C
37000 cP
@Shear Rate 5000 1/s,
Temperature 374 °F
Apparent Dynamic Viscosity
 64000 cP
@Shear Rate 1000 1/s,
Temperature 190 °C
64000 cP
@Shear Rate 1000 1/s,
Temperature 374 °F
Apparent Dynamic Viscosity
 79000 cP
@Shear Rate 300 1/s,
Temperature 190 °C
79000 cP
@Shear Rate 300 1/s,
Temperature 374 °F
Apparent Dynamic Viscosity
Melt Flow 40 g/10 min
@Load 2.16 kg
40 g/10 min
@Load 4.76 lb
Melt flow ratio I10/I2 is 6.8.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 9.80 MPa1420 psi
Tensile Strength, Yield 12.4 MPa1800 psi
Elongation at Break 800 %800 %
Modulus of Elasticity 0.343 GPa49.7 ksiMolded Sample 2% Secant Modulus
Flexural Modulus 0.659 GPa95.6 ksi
Izod Impact, Notched (ISO) 56.0 kJ/m²
@Temperature -50.0 °C
26.6 ft-lb/in²
@Temperature -58.0 °F
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 97.0 °C207 °F
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow DOWLEX™ 2535 Linear Low Density Polyethylene, Narrow MW Distribution
Dow DOWLEX™ 2036A Linear Low Density Polyethylene, Cast Film Grade
Dow DOWLEX™ 2037 Linear Low Density Polyethylene, Cast Film Grade
Dow DOWLEX™ 2056 Linear Low Density Polyethylene, Heavy Duty Film Grade
Dow DOWLEX™ 2500 Linear Low Density Polyethylene, Narrow MW Distribution

PDW455 / 34524

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.