MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ampco Metal AMPCOLOY® 95 Cobalt-Copper Alloy, Extrusion, >50.8 mm.
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Applications: AMPCOLOY 95 finds its own applications due to its slightly higher mechanical properties. AMPCOLOY 95 is principally used for spot welding electrodes, electrodes for mesh welding, electrode holders and seam welding discs for stainless steel, Monel and nickel alloys, flash welding dies, plunger tips in aluminum high pressure die casting machines and parts for injection moulding of plastic wherever a high thermal conductivity is desirable.

Key Words: CDA C17500; RWMA Class 3; ISO NFA 82100; EN CW 103C Typ A3/1; DIN 17666 W. Nr. 2.1285; AFNOR UK2Be
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.75 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 217HB 30
Hardness, Rockwell B 96
Tensile Strength, Ultimate 723 MPa
Tensile Strength, Yield 517 MPa
@Strain 0.5 %
Elongation at Break 17 %
Modulus of Elasticity 130 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000333 ohm-cm52% I.A.C.S.
 
Thermal PropertiesOriginal ValueComments
CTE, linear 17.0 µm/m-°C
@Temperature 20.0 °C
Specific Heat Capacity 0.420 J/g-°C
Thermal Conductivity 208 W/m-K
 
Component Elements PropertiesOriginal ValueComments
Beryllium, Be 0.50 %
Co + Ni 2.0 %
Copper, Cu 97 - 97.5 %As Balance
Other, total <= 0.50 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ampco Metal AMPCOLOY® 83 Beryllium Copper, Extrusion
Ampco Metal AMPCOLOY® 95 Cobalt-Copper Alloy, Extrusion, < 50.8 mm.
Ampco Metal AMPCOLOY® 88 Beryllium Copper, Extrusion
Ampco Metal AMPCOLOY® 89 Beryllium Copper, Extrusion
Ampco Metal AMPCOLOY® 91 Beryllium Copper, Extrusion <35mm

NAMPCO45 / 14999

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.