MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Abatron AboThane 8003-3 Polyurethane Coating
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: AboThane 8003-3 is a clear one-package, moisture-cure polyurethane coating for hardwood, concrete and seamless floors. It was designed for high flexibility, excellent wear and antiskid properties, and abrasion, chemical and corrosion resistance.

Suggested Uses: Floors in warehouses, factories, chemical and food processing plants, gymnasiums, laboratories, clinics, hospitals, classrooms, offices, stores, RR boxcars, seamless floors, aircraft and missile plants, homes and garages, restaurants, and etc.

Information provided by Abatron.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.00 lb/gal
Solids Content 40 %
Viscosity 60 - 125 cP
@Temperature 25.0 °C
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 150 %Direction not specified
Impact Test >= 160 in-lb
Taber Abrasion, mg/1000 Cycles 10S17, 1000 g load
Film Tensile Strength at Break, MD 3500 psiDirection not specified
 
Thermal PropertiesOriginal ValueComments
Flash Point 80.0 °FClosed cup
 
Optical PropertiesOriginal ValueComments
Gardner Color Number <= 1.0
 
Processing PropertiesOriginal ValueComments
Dry Time 2.5 hourTackfree
 12 hourLight traffic ready
 24 hourNormal traffic ready
 
Descriptive Properties
Mandrel FlexibilityPasses 1/8"
Sward Hardness231 day
 261 week

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Thermoset Polyurethane, Adhesive
Abatron KromaKote 8901-8 Polyurethane Coating
Overview of materials for Thermoplastic Polyurethane (TPUR), Polyether Grade
Overview of materials for Thermoplastic Polyurethane, Elastomer, Polyester Grade
Overview of materials for Thermoset Polyurethane, Liquid

PABKW005 / 22046

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.