MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BASF Ultraform® N 2320 003 UNC Q600 POM
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Unreinforced

Material Notes: Ultraform N 2320 003 UNC Q600 is a rapidly solidifying grade of POM for injection molding. Contains a mold release agent.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.40 g/ccISO 1183
Water Absorption 0.80 %ISO 62
Moisture Absorption at Equilibrium 0.20 %23°C/50% R.H.; ISO 62
Melt Flow 8.8 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 145 MPa358/30; ISO 2039-1
Tensile Strength 60.0 MPa
@Time 864000 sec
Hot water storage of tensile bars at 130°C in an autoclave
 61.0 MPa
@Time 450000 sec
Hot water storage of tensile bars at 130°C in an autoclave
 66.0 MPa
@Time 0.000 sec
Hot water storage of tensile bars at 130°C in an autoclave
Tensile Strength, Yield 65.0 MPa50mm/min; ISO 527
 25.0 MPa
@Temperature 120 °C
ISO 527
 35.0 MPa
@Temperature 80.0 °C
ISO 527
 60.0 MPa
@Temperature 40.0 °C
ISO 527
Tensile Stress at Strain 5.00 MPa
@Strain 0.5 %,
Time 3.60e+7 sec
ISO 899-1
 7.00 MPa
@Strain 0.5 %,
Time 360000 sec
ISO 899-1
 10.0 MPa
@Strain 0.5 %,
Time 3600 sec
ISO 899-1
 15.0 MPa
@Strain 2 %,
Time 3.60e+7 sec
ISO 899-1
 17.0 MPa
@Strain 1.5 %,
Time 360000 sec
ISO 899-1
 19.0 MPa
@Time 3600 sec,
Strain 1 %
ISO 899-1
 25.0 MPa
@Strain 4 %,
Time 3.60e+7 sec
ISO 899-1
 29.0 MPa
@Strain 3 %,
Time 360000 sec
ISO 899-1
 31.0 MPa
@Time 3600 sec,
Strain 2 %
ISO 899-1
Elongation at Break 27 %50mm/min; ISO 527
Elongation at Yield 9.4 %50mm/min; ISO 527
Modulus of Elasticity 2.70 GPaISO 527
 1.00 GPa
@Temperature 80.0 °C
ISO 899-1
 1.90 GPa
@Temperature 60.0 °C
ISO 899-1
 3.00 GPa
@Temperature 20.0 °C
ISO 899-1
Tensile Modulus 2.41 GPa
@Thickness 1.50 mm,
Temperature 30.0 °C
 2.59 GPa
@Thickness 4.00 mm,
Temperature 30.0 °C
 2.60 GPa
@Thickness 1.50 mm,
Temperature 90.0 °C
 2.71 GPa
@Thickness 4.00 mm,
Temperature 90.0 °C
 2.79 GPa
@Thickness 1.50 mm,
Temperature 120 °C
 2.81 GPa
@Thickness 4.00 mm,
Temperature 120 °C
Izod Impact, Notched (ISO) 5.50 kJ/m²ISO 180/A
 6.00 kJ/m²ISO 180/A
Charpy Impact Unnotched 21.0 J/cm²ISO 179
 19.0 J/cm²
@Temperature -30.0 °C
ISO 179
Charpy Impact, Notched 0.600 J/cm²ISO 179
 0.550 J/cm²
@Temperature -30.0 °C
ISO 179
Tensile Creep Modulus, 1000 hours 1400 MPaISO 899
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+13 ohm-cmIEC 60093
Surface Resistance 1.00e+13 ohmIEC 60093
Dielectric Constant 3.8
@Frequency 100 Hz
IEC 60250
 3.8
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 40.0 kV/mmIEC 60243-1
Dissipation Factor 0.0010
@Frequency 100 Hz
IEC 60250
 0.0050
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 VTest Solution A; IEC 60112
 600 VTest Solution B; IEC 60112
 
Thermal PropertiesOriginal ValueComments
Melting Point 167 °C
Deflection Temperature at 1.8 MPa (264 psi) 100 °CISO 75
Vicat Softening Point 150 °C(50 °C/h / 50N) - B/50; ISO 306
 
Processing PropertiesOriginal ValueComments
Melt Temperature 190 - 230 °CInjection-molding
Mold Temperature 60.0 - 120 °C
 
Compliance PropertiesOriginal ValueComments
FDA Yes21 CFR 177.2470
NSF YesNSF Std. 51
 YesNSF Std. 61
 
Descriptive Properties
ColorNatural
Commercial StatusActive America
Impact ModifiedNo
Primary Processing TechniqueInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultraform® H 2320 006 Q600 POM
BASF Ultraform® H 4320 Q600 POM
BASF Ultraform® N2320 006 POM
BASF Ultraform® N 2310P Q600 POM
BASF Ultraform® W 2320 003 UNC Q600 POM

PBASF9103 / 84867

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.