MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ferro CeZrO2 Grinding Media
Categories: Ceramic; Oxide; Zirconium Oxide; Other Engineering Material; Grinding/Polishing Media

Material Notes: Grinding media. CeZrO2 has a packing density of 3.72 g/cm³ (232.0 lbs./ft³). Manufactured in East Liverpool and Shreve, Ohio. Data provided by the manufacturer, Ferro Corporation.

Key Words: ceramic cylinders, ZrO2, zirconia, zirconium oxides, ceramic balls, ceramic spheres
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Apparent Bulk Density 6.00 g/ccASTM C20-87
Open Porosity 0.00 %Apparent porosity. ASTM-C20-87
 
Mechanical PropertiesOriginal ValueComments
Vickers Microhardness 1150ASTM E384-89
Modulus of Elasticity 230.5 GPaASTM C674-88
Flexural Strength 806.7 MPaASTM C674-88
Compressive Strength 2440.8 MPaASTM C773-88
Fracture Toughness 8.60 MPa-m½Vickers indentation

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BACT DLC Diamond-Like Coating
A-Glass Fiber, Generic
MarkeTech Gallium Phosphide Semiconductor Wafer, n-type, Sulfur + Tellurium Doped, Czochralski-LEC Grown
Ferro Aluminum Oxide Grinding Media P87
Ferro Aluminum Oxide Grinding Media P70

CFC006 / 804

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.