MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Bohler-Uddeholm UDDEHOLM ELMAX® Powder Metallurgy Stainless Mold Steel
Categories: Metal; Ferrous Metal; Stainless Steel; Tool Steel; Mold Steel

Material Notes: High chromium-vanadium-molybdenum alloyed steel

A through-hardening corrosion resistant mold steel made by powder metallurgy processing techniques. The high wear resistance makes ELMAX® suitable for long production runs; e.g. electronic parts.

ELMAX® is characterized by:

  • High wear resistance
  • High compressive strength
  • Corrosion resistant
  • Very good dimensional stability
Applications: New types of engineering plastics, with high filler contents, place greater demands on the tooling material, in terms of wear resistance and corrosion resistance. Uddeholm Elmax has been specially developed for high-tech applications. These include products within the electronic industry such as connectors, plugs, switches, resistors, integrated circuits, etc. Uddeholm Elmax can also be used in the food processing industry and for industrial and custom knives, where a combination of corrosion resistance and wear resistance is required

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.282 lb/in³hardened to 58 HRC
 0.277 lb/in³
@Temperature 400 °C
hardened to 58 HRC
 0.280 lb/in³
@Temperature 200 °C
hardened to 58 HRC
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 250Soft annealed (Delivery condition)
Hardness, Rockwell C 48 - 62tempering temp 210 - 1110°F
Tensile Strength, Yield 260000 psi
@Strain 0.2 %
hardened to 50 RC
 310000 psi
@Strain 0.2 %
hardened to 55 RC
 335000 psi
@Strain 0.2 %
hardened to 60 RC
Modulus of Elasticity 34800 ksi(hardened to 58 HRC)
 31900 ksi
@Temperature 400 °C
hardened to 58 HRC
 33400 ksi
@Temperature 200 °C
hardened to 58 HRC
Compressive Yield Strength 2300 MPa0.2%, hardened to 50 RC
 2700 MPa0.2%, hardened to 55 RC
 3000 MPa0.2%, hardened to 60 RC
 
Thermal PropertiesOriginal ValueComments
CTE, linear 6.00 µin/in-°F
@Temperature 200 °C
hardened to 58 HRC
 6.50 µin/in-°F
@Temperature 400 °C
hardened to 58 HRC
Specific Heat Capacity 0.110 BTU/lb-°F
@Temperature 20.0 °C
hardened to 58 HRC
Thermal Conductivity 21.0 W/m-K
@Temperature 200 °C
hardened to 58 HRC
 23.0 W/m-K
@Temperature 400 °C
hardened to 58 HRC
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 1.7 %
Chromium, Cr 18 %
Iron, Fe 75.2 %as balance
Manganese, Mn 0.30 %
Molybdenum, Mo 1.0 %
Silicon, Si 0.80 %
Vanadium, V 3.0 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Bohler-Uddeholm UDDEHOLM RAMAX® LH Plastic Mold Steel
Bohler-Uddeholm BÖHLER M303 EXTRA Plastic Mold Steel
Bohler-Uddeholm POLMAX® 420 Modified - Stainless Mold Steel
Bohler-Uddeholm UDDEHOLM CORRAX® Precipitation Hardening Stainless Mold Steel
Chromium Nitride (CrN) PVD Coating

NBUCOR24 / 15493

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.