MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Nurel Engineering Polymers Promyde® B930 P Nylon 6, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced

Material Notes: For transparent applications requiring chemical resistance and mechanical strength.

Information provided by Nurel® Engineering Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.11 g/cc0.0401 lb/in³ISO 1183
Moisture Absorption 3.00 %3.00 %50% RH; ISO 62
Water Absorption at Saturation 9.50 %9.50 %ISO 62
Viscosity Number 125 cm³/g1.25 dl/gISO 307
Linear Mold Shrinkage, Flow 0.00800 - 0.0100 cm/cm0.00800 - 0.0100 in/in
Linear Mold Shrinkage, Transverse 0.00700 - 0.00900 cm/cm0.00700 - 0.00900 in/in
Melt Flow 180 g/10 min
@Load 5.00 kg,
Temperature 275 °C
180 g/10 min
@Load 11.0 lb,
Temperature 527 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 40.0 MPa5800 psi50 mm/min; ISO 527-1/-2
Elongation at Break 1.50 %1.50 %50 mm/min; ISO 527-1/-2
Elongation at Yield 1.50 %1.50 %50 mm/min; ISO 527-1/-2
Tensile Modulus 2.50 GPa363 ksi1 mm/min; ISO 527-1/-2
Flexural Strength 210 MPa30500 psi2 mm/min; ISO 178
Flexural Modulus 2.20 GPa319 ksi2 mm/min; ISO 178
Charpy Impact Unnotched 11.5 J/cm²54.7 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 0.400 J/cm²1.90 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cmISO 60093
Surface Resistance 1.00e+13 ohm1.00e+13 ohmISO 60093
Dielectric Constant 3.50
@Frequency 1.00e+6 Hz
3.50
@Frequency 1.00e+6 Hz
ISO 60250
Dissipation Factor 0.0300
@Frequency 1.00e+6 Hz
0.0300
@Frequency 1.00e+6 Hz
ISO 60250
Comparative Tracking Index 600 V600 VISO 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 70.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
38.9 µin/in-°F
@Temperature 73.4 - 176 °F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 100 µm/m-°C
@Temperature 23.0 - 80.0 °C
55.6 µin/in-°F
@Temperature 73.4 - 176 °F
ISO 11359-1/-2
Melting Point 210 °C410 °FISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 55.0 °C131 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C122 °FISO 75-1/-2
Flammability, UL94 V-2
@Thickness 1.50 mm
V-2
@Thickness 0.0591 in
Glow Wire Ignition Temperature 675 °C
@Thickness 1.50 mm
1250 °F
@Thickness 0.0591 in
IEC 60695-2-12,12
Glow Wire Flammability Index 800 °C
@Thickness 1.50 mm
1470 °F
@Thickness 0.0591 in
IEC 60695-2-12,12
 
Processing PropertiesMetricEnglishComments
Melt Temperature 220 - 290 °C428 - 554 °FInjection Molding
Mold Temperature 0.000 - 30.0 °C32.0 - 86.0 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNUREL9010 / 327227

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.