MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Chengdu Polyster KLX-G11 PC Film & Sheet
Categories: Polymer; Film; Thermoplastic; Polycarbonate (PC)

Material Notes: PC film and sheet, high transparency, both sides are polished, both sides with transparent protective films. Is printable, flame-retardant, anti-static, resists ultraviolet decay, scratch resistant, sunglass, sunbonnet, electroplate, .

Information provided by Chengdu Polyster Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/ccISO 1183
Water Absorption 0.20 %23 to 24 hours; ASTM D570
Thickness 0.125 - 1.00 mil
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 75ASTM D2240
Tensile Strength, Ultimate 60.0 MPaASTM D882
Elongation at Break 140 %ASTM D882
Flexural Strength 90.0 MPaASTM D790
Izod Impact, Notched 700 - 860 J/mIzod tape gap; ASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+16 ohm-cmASTM D257
Surface Resistance 1.00e+15 ohmASTM D257
Dielectric Strength 30.0 kV/mm
@Thickness 1.60 mm
ASTM D149
Arc Resistance 110 secASTM D495
 
Thermal PropertiesOriginal ValueComments
CTE, linear 70.0 µm/m-°C
@Temperature 20.0 °C
ASTM D696
Thermal Conductivity 0.190 W/m-KASTM D117
Maximum Service Temperature, Air 110 °C
Flammability, UL94 V-2
@Thickness 0.400 mm
Shrinkage 0.50 - 0.70 %
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.585ASTMD542
Haze 3.0 %
@Thickness 1.00 mm
ASTMD1003
Transmission, Visible 89 %
@Thickness 1.00 mm
ASTMD1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Elektro-Isola G-Etronax EP FR4 Epoxy, Glass Fabric Reinforcement, Light Yellow, Sheets
Polymer Resources PPX-FR4 Modified-PPO, V-1 Flame Retardant
G-11 Fiberglass Epoxy Laminate Sheet
Beijing Ranger Chem PBT-201-G10 Flame Retarding FR PBT
Beijing Chemical Industry KAIFA® MN201-G10 Nylon 66 Resin

PCHEN002 / 79299

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.