MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
DuPont Mobility and Materials Hytrel® HTR8139BK TPC-ET  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyester TPE

Material Notes: 44 Shore D, Lubricated, High Viscosity Polyester Elastomer Developed for Blow Molding

While this product line has been acquired by Celanese, this specific grade had been disconued while still a DuPont product so it is listed here as a discontinued DuPont product.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.15 g/ccISO 1183
Melt Density 0.960 g/cc
@Temperature >=194 °C
Water Absorption 0.70 %
@Time 86400 sec
Sim. to ISO 62
 0.70 %
@Thickness 2.00 mm
Sim. to ISO 62
Moisture Absorption 0.200 %
@Thickness 2.00 mm
Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.016 cm/cmISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.014 cm/cmISO 294-4, 2577
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
from MVR and melt density; ISO 1133
 2.1 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 44ISO 7619-1
 40
@Time 15.0 sec
ISO 7619-1
Tensile Strength at Break 32.0 MPaISO 527-1/-2
Tensile Stress at Strain 4.50 MPa
@Strain 5.0 %
ISO 527-1/-2
 6.70 MPa
@Strain 10 %
ISO 527-1/-2
 11.8 MPa
@Strain 50 %
ISO 527-1/-2
 14.0 MPa
@Strain 100 %
ISO 527-1/-2
 23.0 MPa
@Strain 300 %
ISO 527-1/-2
Elongation at Break >= 300 %ISO 527-1/-2
 510 %ISO 527-1/-2
Tensile Modulus 55.0 MPaISO 527-1/-2
Flexural Modulus 87.0 MPaISO 178
Izod Impact, Unnotched (ISO) NB
@Temperature 23.0 °C
ISO 180/1A
 NB
@Temperature -40.0 °C
ISO 180/1A
Charpy Impact Unnotched NB
@Temperature 23.0 °C
ISO 179/1eU
 NB
@Temperature -30.0 °C
ISO 179/1eU
Charpy Impact, Notched NB
@Temperature 23.0 °C
ISO 179/1eA
 NB
@Temperature -30.0 °C
ISO 179/1eA
 NB
@Temperature -40.0 °C
ISO 179/1eA
Tear Strength 110 kN/mparallel; ISO 34-1
 120 kN/mnormal; ISO 34-1
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 4.00e+13 ohm-cmIEC 62631-3-1
Surface Resistance >= 1.00e+15 ohmIEC 62631-3-2
Dielectric Constant 4.6
@Frequency 1e+6 Hz
IEC 62631-2-1
 4.9
@Frequency 100 Hz
IEC 62631-2-1
Dielectric Strength 19.0 kV/mmIEC 60243-1
Dissipation Factor 0.0050
@Frequency 100 Hz
IEC 62631-2-1
 0.0275
@Frequency 1e+6 Hz
IEC 62631-2-1
Comparative Tracking Index 600 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 180 µm/m-°CISO 11359-1/-2
 210 µm/m-°C
@Temperature -40.0 - 23.0 °C
ISO 11359-1/-2
CTE, linear, Transverse to Flow 170 µm/m-°CISO 11359-1/-2
 200 µm/m-°C
@Temperature -40.0 - 23.0 °C
ISO 11359-1/-2
Melting Point 194 °C10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 58.0 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 44.0 °CISO 75-1/-2
Brittleness Temperature -100 °CISO 974
Glass Transition Temp, Tg -45.0 °C10°C/min; ISO 11357-1/-2
Flame Spread <= 80.0 mm/min
@Thickness 1.00 mm
ISO 3795 (FMVSS 302)
Oxygen Index 21 %ISO 4589-1/-2
 
Processing PropertiesOriginal ValueComments
Melt Temperature 225 °CInjection Optimum
 220 - 240 °CInjection
Mold Temperature 40.0 - 50.0 °CInjection
 45.0 °CInjection Optimum
Drying Temperature 100 °CInjection
Dry Time 2.00 - 4.00 hourDehumidified Dryer; Injection
Moisture Content 0.080 %Injection
 
Descriptive Properties
AdditivesLubricants
Delivery formPellets
Drying RecommendedyesInjection
Eff. thermal diffusivity5.44E-08 m²/s
FMVSS ClassBISO 3795 (FMVSS 302)
Part Marking CodeTPC-ETISO 11469
ProcessingBlow Molding
 Injection Molding
 Thermoforming
Regional AvailabilityAsia Pacific
 Europe
 Global
 Near East/Africa
 North America
 South and Central America
Resin IdentificationTPC-ETISO 1043
Special characteristicsHeat stabilized or stable to heat
 Light stabilized or stable to light

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Hytrel® HTR8223 BK320 TPC-ET
Celanese Hytrel® 4556 TPC-ET
Celanese Hytrel® 6356 TPC-ET
Celanese Hytrel® HTR8068 TPC-ET-FR(17)
Celanese Hytrel® 4053FG NC010 TPC-ET

PDSX5208 / 197848

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.