MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Phillips 66 Omniguard® 460 NLGI Grade 2
Categories: Fluid; Lubricant; Calcium Gellant

Material Notes: Omniguard 460 is a premium quality, multipurpose, extreme pressure (EP) calcium sulfonate grease specially developed for use in industrial and automotive equipment operating under severe conditions involving high loads, high temperatures and/or wet environments. Omniguard 460 is manufactured with high-quality base oils, a special polymer and a non-soap, calcium sulfonate thickener. It is fortified with antiwear additives and rust and corrosion inhibitors. It protects against rust and corrosion in high-humidity, high-temperature applications such as those found in the steel, lumber, tire manufacturing and paper industries. It has outstanding resistance to water washout, excellent load-carrying capacity to protect against wear, and outstanding shear stability to resist mechanical breakdown.

Applications:

  • Industrial equipment operating under unfavorable conditions involving water contamination, high loads and/or high temperatures
  • Plain and rolling-element bearings operating in corrosive environmental conditions
  • Rolling mills, hot roll tables, continuous casters, ingot buggies and slab mills
  • Steel mill roller bearings, conveyors and gears
  • Marine and heavy mobile equipment exposed to salt water
  • Paper machine wet-and dry-end bearings and hot calendar stacks
  • Automotive wheel bearings and chassis parts
Features/Benefit:
  • Excellent oxidation resistance and thermal stability at high temperatures
  • Outstanding rust and corrosion protection, including resistance to saltwater corrosion
  • Excellent extreme-pressure and antiwear properties
  • Outstanding resistance to water washout
  • Outstanding shear stability
  • Good adhesion to metal surfaces
  • High dropping point (>550°F)
  • Does not contain heavy metals or other environmentally undesirable components

Information provided by Phillips 66 Lubricants.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.39 lb/gal
Viscosity Measurement 94Index
Saybolt Viscosity at 100°F 2470 SUS
Saybolt Viscosity at 210°F 147 SUS
Kinematic Viscosity at 40°C (104°F) 460 cSt
Kinematic Viscosity at 100°C (212°F) 30 cSt
Oxidative Stability 100 hour
@Pressure 0.000 MPa
Pressure Drop; ASTM D942
 
Mechanical PropertiesOriginal ValueComments
Four Ball Extreme Pressure, Weld Load 500 kgASTM D2596
Four Ball Wear 0.390 mmScar Diameter; ASTM D2266
Penetration 265 - 295
Timken Test 65.0 lbOK Load; ASTM D2509
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 190 °C
Minimum Service Temperature, Air -29.0 °C
Dropping Point 300 °C
 
Descriptive Properties
ColorTan
Roll Stability0.07Change in Penetration, ASTM D1831
Shear Stability0.02Change (100,000 strokes), ASTM D217
ThickenerCalcium Sulfonate
Water Washout Resistance2.75Weight Loss @ 175°F, ASTM D1264

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WCON5133 / 198386

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.