MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

3D Systems DuraForm® EX Impact-Resistant Plastic for SLS® Systems
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer

Material Notes: This impact-resistant plastic offers the toughness of injection-molded polypropylene and ABS and is suitable for Rapid Manufacturing. For use with all Sinterstation® Pro and Sinterstation HiQ™ series SLS® systems.

    Applications
  • Complex, thin-wall ductwork
    • Motorsports
    • Aerospace
    • Unmanned air vehicles (UAV’s)
  • Housings and enclosures
  • Impellers
  • Connectors
  • Consumer sporting goods
  • Vehicle dashboards and grilles
  • Bumpers
  • Snap-fit designs
  • Living hinges
  • Functional prototypes that require end-use performance properties
  • Appropriate for low- to mid-volume rapid manufacturing

All information provided by 3D Systems.

Vendors:
Proto3000 provides design tools, 3D printers, additive manufacturing processes, metrology technologies, high-performance materials, and part-finishing automation. Our ISO 9001:2015 additive manufacturing production facility offers 3D printing services, rapid prototyping services, and end-part production with HP MultiJet Fusion (MJF), FDM, SLA, SLS, Polyjet, DLP, metal binder jetting, BMD, and DMLS.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.01 g/cc1.01 g/ccASTM D792
Water Absorption 0.48 %
@Time 86400 sec
0.48 %
@Time 24.0 hour
ASTM D570
Water Absorption at Saturation 1.15 %1.15 %ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell L 6969ASTM D785
Hardness, Rockwell M 3434ASTM D785
Hardness, Shore D 7474ASTM D2240
Tensile Strength, Ultimate 48.0 MPa6960 psiASTM D638
Tensile Strength, Yield 37.0 MPa5370 psiASTM D638
Elongation at Break 47 %47 %ASTM D638
Elongation at Yield 5.0 %5.0 %ASTM D638
Tensile Modulus 1.517 GPa220.0 ksiASTM D638
Flexural Strength 26.0 MPa3770 psiUltimate; ASTM D790
Flexural Yield Strength 42.0 MPa6090 psiASTM D790
Flexural Modulus 1.31 GPa190 ksiASTM D790
Izod Impact, Notched 0.740 J/cm
@Temperature 23.0 °C
1.39 ft-lb/in
@Temperature 73.4 °F
ASTM D256
Izod Impact, Unnotched 14.86 J/cm
@Temperature 23.0 °C
27.84 ft-lb/in
@Temperature 73.4 °F
ASTM D256
Gardner Impact 11.8 J8.70 ft-lbASTM D5420
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.30e+13 ohm-cm1.30e+13 ohm-cmASTM D257
Surface Resistance 4.90e+12 ohm4.90e+12 ohmASTM D257
Dielectric Constant 4.5
@Frequency 1000 Hz
4.5
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 18.5 kV/mm470 kV/inASTM D149
Dissipation Factor 0.050
@Frequency 1000 Hz
0.050
@Frequency 1000 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear  120 µm/m-°C
@Temperature 0.000 - 50.0 °C
66.7 µin/in-°F
@Temperature 32.0 - 122 °F
ASTM E831
 342 µm/m-°C
@Temperature 85.0 - 145 °C
190 µin/in-°F
@Temperature 185 - 293 °F
ASTM E831
Specific Heat Capacity 1.75 J/g-°C0.418 BTU/lb-°FASTM E1269
Thermal Conductivity 0.510 W/m-K3.54 BTU-in/hr-ft²-°FASTM E1225
Deflection Temperature at 0.46 MPa (66 psi) 188 °C370 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 48.0 °C118 °FASTM D648
Flammability, UL94 HBHB

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3D Systems DuraForm® PA Nylon for SLS® Systems
CRP Technology Windform® RL Thermoplastic Elastomer for SLS
Overview of materials for Polypropylene, Molded
3D Systems DuraForm® HST Fiber Filled Nylon for SLS Systems
3D Systems DuraForm® Flex Thermoplastic Elastomer for SLS® Systems

PAPPR118 / 83497

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.