System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Epsan Epimix PBT GFR 30 NC Q1D001 Polybutylene Terephthalate
Categories:
Polymer
;
Thermoplastic
;
Polyester, TP
;
Polybutylene Terephthalate (PBT)
;
Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled
Material Notes:
EPIMIX PBT, reinforced with 30% of glass fiber, heat stabilized, superior gloss, lubricated for injection molding. EPIMIX PBT GFR 30 is used in all sectors of industry, compliance with RoHs derivatives.
Information provided by Epsan Plastik
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.52
g/cc
ISO 1183
Linear Mold Shrinkage
0.0030
cm/cm
Parallel; ISO 294-4
0.010
cm/cm
Normal; ISO 294-4
Ash
30 %
ISO 3451-4
Mechanical Properties
Original Value
Comments
Tensile Stress
120
MPa
ISO 527-2
Elongation at Break
2.0 %
ISO 527-2
Tensile Modulus
8200
MPa
ISO 527-2
Flexural Strength
110
MPa
ISO 178
Flexural Modulus
7800
MPa
ISO 178
Izod Impact, Notched (ISO)
7.00
kJ/m²
ISO 180/1A
Charpy Impact, Notched
8.00
kJ/m²
ISO 179/1eA
Thermal Properties
Original Value
Comments
Melting Point
220
°C
ISO 3146
Deflection Temperature at 0.46 MPa (66 psi)
214
°C
ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi)
210
°C
ISO 75-2/A
Vicat Softening Point
214
°C
ISO 306/B50
Flammability, UL94
HB
@Thickness 1.60 mm
EN 60695-11-10
Processing Properties
Original Value
Comments
Processing Temperature
260
°C
Recommended Injection Molding Temperature
Drying Temperature
80.0
°C
Average Drying Time is 2-4 hrs
Moisture Content
0.20 %
ISO 15512
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Epsan Epimix PBT NC Q101 Polybutylene Terephthalate
Epsan Epimix PBT IMP NC Q1B801 Polybutylene Terephthalate
Epsan Epimix PBT GV0 30 NC Q1D0B301 Polybutylene Terephthalate
Epsan Epimix PBT GV0 10 NC Q1B0B501 Polybutylene Terephthalate, Halogenated
Epsan Epimix PBT GFR 10 NC Q1B001 Polybutylene Terephthalate
PEPSAN074 / 186388
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.