MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Guang Dong LH-PP813 Conductive PP
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Application Field: Drawing class, suitable for making wire, flat wire and round wire

Feature: Easy to shape model, good tensile strength, good liquidity and good toughness

Grade: Drawing Level

Information provided by GuangDong LuHua New Material Technology Holding Co

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Melt Flow 0.40 - 1.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
0.40 - 1.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
GB/T3682
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 27.0 - 34.0 MPa3920 - 4930 psiGB/T1040
Flexural Strength 18.0 - 22.0 MPa2610 - 3190 psiGB/T9341
Flexural Modulus 0.968 - 1.15 GPa140 - 167 ksiGB/T9341
Izod Impact, Notched (ISO) 4.50 - 5.50 kJ/m²2.14 - 2.62 ft-lb/in²GB/T1843
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 1.00e+6 - 1.00e+7 ohm1.00e+6 - 1.00e+7 ohmGB/T1410

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGDON016 / 283964

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.