MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Mateck Barium Fluoride, BaF2
Categories: Ceramic; Halide

Material Notes: Optical crystals

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 4.83 g/cc
@Temperature 20.0 °C
0.174 lb/in³
@Temperature 68.0 °F
Solubility 0.17 ppm0.17 ppm
a Lattice Constant 6.196 Å6.196 Å
c Lattice Constant 6.196 Å6.196 Å
Molecular Weight 175.3 g/mol175.3 g/mol
 
Mechanical PropertiesMetricEnglishComments
Vickers Microhardness 820820MPa
Hardness, Mohs 3.03.0
Modulus of Elasticity 65.4 GPa9490 ksi<100> direction
 66.3 GPa9620 ksi<111> direction
Poissons Ratio 0.3070.307
Shear Modulus 25.1 GPa3640 ksi<100> direction
 25.3 GPa3670 ksi<111> direction
 
Thermal PropertiesMetricEnglishComments
CTE, linear 16.5 - 19.2 µm/m-°C
@Temperature -60.0 - 60.0 °C
9.17 - 10.7 µin/in-°F
@Temperature -76.0 - 140 °F
Specific Heat Capacity 0.456 J/g-°C0.109 BTU/lb-°F
Thermal Conductivity 7.10 W/m-K
@Temperature 38.0 °C
49.3 BTU-in/hr-ft²-°F
@Temperature 100 °F
Melting Point 1354 °C2469 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.39261.3926at n10.5
 1.305
@Wavelength 15000 nm
1.305
@Wavelength 15000 nm
 1.4014
@Wavelength 10000 nm
1.4014
@Wavelength 10000 nm
 1.4647
@Wavelength 2000 nm
1.4647
@Wavelength 2000 nm
 1.4759
@Wavelength 546.1 nm
1.4759
@Wavelength 546.1 nm
at ne
 1.5573
@Wavelength 200 nm
1.5573
@Wavelength 200 nm
IR Transmittance  42 %
@Wavelength 12000 nm
42 %
@Wavelength 12000 nm
Internal Transmittance
 97 %
@Wavelength 1000 nm
97 %
@Wavelength 1000 nm
Internal Transmittance
 97 %
@Wavelength 7000 nm
97 %
@Wavelength 7000 nm
Internal Transmittance
UV Transmittance 70 %
@Wavelength 200 nm
70 %
@Wavelength 200 nm
Internal Transmittance
 
Descriptive Properties
Absorption loss (cm^-1)0.08at 0.4 microns
 0.13at 10.6 microns
 0.2at 0.2 microns
Cleavability(111)perfect
Constants of Elastic Compliance (Pa^-1)1.53E-11S11
 39.47S44
 -4.69E-12S12
Symmetrycubic
Symmetry Classm3m
Thermal Coefficient of Refractive Index-1.27E-5 to -1.51E-53.39 microns for ± 60°C
Thermal Stability, °C10±2
Transmission Range (microns)0.15 - 12.5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Sandstone, Hard
Misumi Machinable SiO2-MgO Ceramic
Special Metals INCONEL® Alloy 600
Goodfellow Potassium Aluminosilicate (Muscovite Mica)
Aluminum, Al

CMAT038 / 87722

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.