MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil LD 334.57 Clear, High Impact Film Resin  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate Copolymer (EVA), Film Grade

Material Notes: LD 334 resins produce films with superior impact strength, good heat sealability, and low temperature properties.

Information provided by ExxonMobil Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.924 g/ccExxonMobil Method
Vinyl Acetate Content 4.2 %ExxonMobil Method
Melt Flow 1.25 g/10 minExxonMobil Method
Antiblock Level 4000 ppm
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 1170 psiat 2% offset; ASTM D882
Film Tensile Strength at Yield, TD 1110 psiat 2% offset; ASTM D882
Film Elongation at Break, MD 180 %ASTM D882
Film Elongation at Break, TD 580 %ASTM D882
Film Elongation at Yield, MD 7.0 %ASTM D882
Film Elongation at Yield, TD 5.5 %ASTM D882
Elmendorf Tear Strength MD 170 gASTM D1922
Elmendorf Tear Strength TD 90 gASTM D1922
Dart Drop Test 180 gASTM D1709
Film Tensile Strength at Break, MD 3530 psiASTM D882
Film Tensile Strength at Break, TD 3360 psiASTM D882
1% Secant Modulus, MD 20400 psiASTM D882
1% Secant Modulus, TD 23700 psiASTM D882
 
Thermal PropertiesOriginal ValueComments
Melting Point 220 °FPeak Melting Temperature; ExxonMobil Method
Crystallization Temperature 91.0 °CExxonMobil Method
Vicat Softening Point 189 °FASTM D1525
 
Optical PropertiesOriginal ValueComments
Haze 7.4 %ASTM D1003
Gloss 68 %45°; ASTM D2457
Transmission, Visible 90 %clear; thickness not quantified
 
Descriptive Properties
FeaturesThermal Stabilizer

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil LD 144.50 Packaging Film Resin
ExxonMobil EVA 5008 Low Density Polyethylene Resin
ExxonMobil Escorene® UL-7560 EVA Copolymer, Adhesive and Sealant Grade
ExxonMobil Escorene® MV-02520 EVA Copolymer, Adhesive and Sealant Grade
ExxonMobil Escorene® LD-740 High EVA Film and Compounding Resin

PEXB019 / 37324

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.