MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ametek P410L P/M Stainless Steel, Sintered from 6.0 g/cc Green Density
Categories: Metal; Ferrous Metal; Stainless Steel; T 400 Series Stainless Steel

Material Notes: Powder apparent bulk density 2.8 g/cc; powder flow 30 sec/50g.

Compacting properties measured on powders with 1% lithium stearite. Sintering was done in dissociated ammonia at 1121°C (2050°F) for 45 minutes. Sintered properties below were determined using transverse rupture bars. Compacting pressure 30 tsi. Green strength 1500 psi. Sintered breaking strength 85 ksi. Dimensional change from die size -0.31%.

Information provided by Ametek Specialty Metal Products.

Key Words: Powder metallurgy
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 6.13 g/cc0.221 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 4242
Tensile Strength, Ultimate 280 MPa40600 psi
Elongation at Break 3.6 %3.6 %
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.030 %<= 0.030 %
Chromium, Cr 11.5 - 13.5 %11.5 - 13.5 %
Iron, Fe 83.5 - 88.5 %83.5 - 88.5 %as balance
Manganese, Mn <= 2.0 %<= 2.0 %
Phosphorus, P <= 0.040 %<= 0.040 %
Silicon, Si <= 1.0 %<= 1.0 %
Sulfur, S <= 0.030 %<= 0.030 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ATI Allegheny Ludlum Stainless Steel Type 439/AL 439HP™ (ASTM XM-8; UNS S43035)
MetalTek MTEK 440C Cast UNS J91639 Martensitic Stainless Steel
MetalTek MTEK H46 Martensitic Stainless Steel
Sandvik Osprey 420 Stainless Steel Powder (Grade 80% - 22)
Sandvik Osprey 420/MA Stainless Steel Powder (Grade 80% - 22)

NMA030 / 18139

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.