MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese Zytel® HTNFR52G30BL BK337 PA6T/66-GF30FR(16+72)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6/66; Nylon 66/6, 30% Glass Fiber Reinforced

Material Notes: 30% Glass Reinforced, Flame Retardant, PPA, High Performance Polyamide

Former DuPont product acquired by Celanese in 2022.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.62 g/ccDAM; ISO 1183
Linear Mold Shrinkage, Flow 0.0030 cm/cmDAM; ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0080 cm/cmDAM; ISO 294-4, 2577
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 160 MPaDAM; ISO 527-1/-2
Elongation at Break 2.0 %DAM; ISO 527-1/-2
Tensile Modulus 11800 MPaDAM; ISO 527-1/-2
Flexural Strength 210 MPa50% RH; ISO 178
 240 MPaDAM; ISO 178
Flexural Modulus 10000 MPaDAM; ISO 178
Poissons Ratio 0.33DAM
Charpy Impact Unnotched 35.0 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 179/1eU
 35.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eU
 40.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eU
 50.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eU
Charpy Impact, Notched 10.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eA
 10.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmDAM; IEC 62631-3-1
Dielectric Constant 3.3
@Frequency 1e+6 Hz
DAM; IEC 62631-2-1
 3.5
@Frequency 100 Hz
DAM; IEC 62631-2-1
Dissipation Factor 0.0050
@Frequency 100 Hz
DAM; IEC 62631-2-1
 0.0135
@Frequency 1e+6 Hz
DAM; IEC 62631-2-1
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 20.0 µm/m-°CDAM; ISO 11359-1/-2
 10.0 µm/m-°C
@Temperature 55.0 - 160 °C
DAM; ISO 11359-1/-2
 20.0 µm/m-°C
@Temperature -40.0 - 23.0 °C
DAM; ISO 11359-1/-2
CTE, linear, Transverse to Flow 63.0 µm/m-°CDAM; ISO 11359-1/-2
 57.0 µm/m-°C
@Temperature -40.0 - 23.0 °C
DAM; ISO 11359-1/-2
 100 µm/m-°C
@Temperature 55.0 - 160 °C
DAM; ISO 11359-1/-2
Melting Point 310 °Cfirst heat; DAM; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 282 °CDAM; ISO 75-1/-2
Glass Transition Temp, Tg 45.0 °C10°C/min; 50% RH; ISO 11357-1/-2
 90.0 °C10°C/min; DAM; ISO 11357-1/-2
Flammability, UL94 V-0
@Thickness 1.50 mm
DAM; IEC 60695-11-10
 V-0
@Thickness 3.00 mm
DAM; IEC 60695-11-10
 5VA
@Thickness 1.50 mm
DAM; IEC 60695-11-20
Oxygen Index 42 %DAM; ISO 4589-1/-2
Glow Wire Ignition Temperature 925 °C
@Thickness 0.750 mm
DAM; IEC 60695-2-13
 925 °C
@Thickness 1.50 mm
DAM; IEC 60695-2-13
 960 °C
@Thickness 3.00 mm
DAM; IEC 60695-2-13
 
Processing PropertiesOriginal ValueComments
Melt Temperature 325 °COptimum, Injection
 320 - 330 °CRange, Injection
Mold Temperature 90.0 - 110 °CInjection
Drying Temperature 100 °CInjection
Dry Time 6.00 - 8.00 hourInjection, Dehumidified Dryer
Moisture Content <= 0.10 %Injection
 
Descriptive Properties
AdditivesFlame retardant
Drying RecommendedyesInjection
Emission of organic compounds (µgC/g)35VDA 277
FMVSS ClassDNIISO 3795 (FMVSS 302)
Fogging (%)95F-value (refraction); ISO 6452; DAM
ISO designationISO 16396-PA6T/66,GF30 FR(16+72),M1CF1GR,S10-120
Odor Class4.5VDA 270
Part Marking Code>PA6T/66-GF30FR(16+72)<ISO 11469
 >PPA-GF30FR<SAE J1344
PolymerPA6T/66-GF30 FR(16+72)
Resin IdentificationPA6T/66-GF30FR(16+72)ISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Zytel® HTNFR52G30BL NC010 PA6T/66-GF30FR(16+72)
Celanese Zytel® FR50 BK505 PA66-GF25FR(17)
Celanese Zytel® HTNFR52G30NH BK337 PA6T/66-GF30FR(40)
Celanese Zytel® HTNFR52G30NH NC010 PA6T/66-GF30FR(40)
Celanese Zytel® 101 NC010 PA66

PDSX5462 / 198102

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.