MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil Escorene™ FL 00328 Ethylene Vinyl Acetate Copolymer (European Grade)
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate

Material Notes: Product Description: FL 00328 is a copolymer of ethylene and vinyl acetate offering low gel.
Processing Conditions: Processing temperatures above 220°C (428°F) may cause resin degradation. Machines should always be completely purged with LDPE or suitable cleaning compound before shutdown.

Availability: Africa & Middle East, Asia Pacific and Europe

Additive:

  • Antiblock: No
  • Slip: No
  • Thermal Stabilizer: No
Applications:
  • Co-Extrusion Films
  • Compounding
  • Fabric Coating
  • Sheet Extrusion

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.951 g/ccExxonMobil method
Vinyl Acetate Content 27 %ExxonMobil method
Melt Flow 3.0 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 81
@Time 15.0 sec
Molded Properties; ISO 868
Tensile Strength at Break >= 100 psiMolded Properties; ISO 527-2/1A/100
Tensile Modulus 2300 psiMolded Properties; ISO 527-2/1
 
Thermal PropertiesOriginal ValueComments
Melting Point <= 160 °FPeak Melting Point; ExxonMobil method
Vicat Softening Point 112 °FASTM D1525
 
Descriptive Properties
Blending Temperature220

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Arkema EVATANE® 28-05 Copolymer Ethylene - Vinyl Acetate
Arkema EVATANE® 28-03 Copolymer Ethylene - Vinyl Acetate
ExxonMobil EVA 1718.CC3 Ethylene Vinyl Acetate Copolymer (European Grade)
ExxonMobil Escorene™ AD 0633EH2 Ethylene Vinyl Acetate Copolymer (European Grade)
ExxonMobil Escorene™ FL 00714 Ethylene Vinyl Acetate Copolymer (European Grade)

PEX99092 / 175328

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.