System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Evonik Vestamid® L2170 Nylon 12
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 12 (PA12)
Material Notes:
Description:
High-viscosity, heat- and highly light-stabilized, with processing aid
Applications:
UV-stable and termite-resistant cable sheathing
Information provided by degussa.
Evonik Industries is the successor company to Degussa.
Key Words:
PA12, EHL,22-010
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.01
g/cc
ISO 1183
Moisture Absorption at Equilibrium
0.70 %
@Thickness 1.00 mm,
Temperature 23.0 °C
50% R.H.; ISO 62
Water Absorption at Saturation
1.6 %
@Thickness 1.00 mm
ISO 62
Linear Mold Shrinkage
0.012
cm/cm
127x12.7x3.2 mm (processing cond. acc. To ISO 1874-2)
Linear Mold Shrinkage, Transverse
0.014
cm/cm
127x12.7x3.2 mm (processing cond. acc. To ISO 1874-2)
Mechanical Properties
Original Value
Comments
Tensile Strength, Yield
47.0
MPa
ISO 527-1/2
Elongation at Break
>= 50 %
ISO 527-1/2
Elongation at Yield
5.0 %
ISO 527-1/2
Tensile Modulus
1.40
GPa
ISO 527-1/2
Charpy Impact Unnotched
NB
@Temperature -30.0 °C
ISO 179/1eU
NB
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched
0.900
J/cm²
@Temperature -30.0 °C
ISO 179/1eA
1.60
J/cm²
@Temperature 23.0 °C
ISO 179/1eA
Electrical Properties
Original Value
Comments
Volume Resistivity
1.00e+15
ohm-cm
IEC 60093
Dielectric Constant
3.0
@Frequency 1e+6 Hz
IEC 60250
3.7
@Frequency 100 Hz
IEC 60250
Dielectric Strength
26.0
kV/mm
K20/P50; IEC 60243-1
Dissipation Factor
0.026
@Frequency 1e+6 Hz
IEC 60250
0.045
@Frequency 100 Hz
IEC 60250
Comparative Tracking Index
>=
600
V
Test Solution A, 50 drops; IEC 60112
600
V
Test Solution A, 100 drops; IEC 60112
Thermal Properties
Original Value
Comments
CTE, linear
140
µm/m-°C
@Temperature 23.0 - 55.0 °C
45x15x10 mm; ISO 11359
Melting Point
178
°C
Peak Temperature; ISO 3146, ISO 11357
Deflection Temperature at 0.46 MPa (66 psi)
110
°C
ISO 75
Deflection Temperature at 1.8 MPa (264 psi)
50.0
°C
ISO 75
Vicat Softening Point
140
°C
50N; ISO 306
170
°C
10N; ISO 306
Flammability, UL94
HB
@Thickness 1.60 mm
HB
@Thickness 3.20 mm
Descriptive Properties
Electrolytic Corrosion
A1 Step
IEC 60426
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Evonik Vestamid® L2140 Nylon 12
Evonik Vestamid® L1940 Nylon 12
Evonik VESTAMID® HTplus M1000 PA6T/X
Evonik Vestamid® L1670 Nylon 12 for Fiber Optic Jacketing
Evonik Vestamid® X7373 Nylon 12
PHULA40 / 47400
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.