MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Covestro Bayfol® CR 1-4 000000 Polycarbonate + PBT  (discontinued **)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced; Polyester, TP; Polybutylene Terephthalate (PBT)

Material Notes: Characterization: Bayfol CR 1-4 000000 is an extrusion film based on Makrolon® (PC)/ Polyester (PBT) blend.

Properties / Applications: Bayfol CR 1-4 000000 has advantages over standard polycarbonate films in terms of dynamic strength, dimensional stability and cold formability. Typical applications are automotive, keypads, membrane switches, hand held electronics, appliance, nameplates, touch panels and FIM - film insert molding decoration. Bayfol CR 1-4 000000 is available in various standard thicknesses from 0.005 ” to 0.015 ” (125 microns to 375 microns). Other thicknesses are available on request. The surface combination of Bayfol CR 1-4 000000 is one side gloss and one side fine matte for printability. As with any product, use of Bayfol CR 1-4 000000 in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.23 g/ccASTM D792
Water Absorption 0.35 %
@Time 86400 sec
Immersion; ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 55.8 MPaASTM D882
Tensile Strength, Yield 8650 psiASTM D882
Elongation at Break 125 %ASTM D882
Tear Strength 960 pliInitiation; ASTM D1004
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 80.0 µm/m-°C
@Temperature 20.0 - 120 °C
DIN 53752
CTE, linear, Transverse to Flow 80.0 µm/m-°C
@Temperature 20.0 - 120 °C
DIN 53752
Shrinkage <= 0.30 %
@Temperature 90.0 °C,
Time 3600 sec
transverse; IEC 60674-2
 <= 0.40 %
@Temperature 90.0 °C,
Time 3600 sec
parallel; IEC 60674-2
 
Optical PropertiesOriginal ValueComments
Haze 92 %ASTM D1003
Gloss >= 90 %60° top side, black inked second surface; ASTM D2457
Yellow Index 1.0 %ASTM E313
Transmission, Visible >= 80 %ASTM D1003
 
Descriptive Properties
AvailabilityEurope
 Near East/Africa
 North America
 South and Central America

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Bayfol® AS-A 2-4 Polycarbonate + PBT
A. Schulman Lucent PC/PBT-0820 Polycarbonate+PBT, Injection Grade
Covestro Bayfol® CR 6-2 000000 Polycarbonate + PBT
Covestro Makroblend® DP 6015 Polycarbonate + PBT
Covestro Makroblend® UT5205 PC/PBT Blend

PB09747 / 92587

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.