Kaowool HS is a high strength product recommended for tough mechanical stress areas. Also, very good for back-up behind dense refractories. Features: Excellent thermal conductivity Capability to withstand chemical attack Board capabilities are 48 x 36 x 1/4 to 3" (120 x 90 x 0.625 to 7.5 cm) with the exception of PM Board which can be made 1/8" (3.125 cm) thick Applications: Appliance and heat processing insulation Back up in steel ladle and torpedo cars Backup insulation to dense refractories Combustion chamber construction Expansion joint material Flue and chimney linings Furnace, kiln, and oven hot face linings General molten metal contact Glass coffin walls Glass regenerator insulation Glass tank side, end wall and port neck Glass tank wall and port neck insulation Heat shields High temperature gaskets and seals High mechanical stress areas Kiln furniture Trough linings in contact with aluminumInformation provided by Thermal Ceramics Data has not been recently verified. Please contact manufacturer for current information. |