MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
DuPont Teijin Films Melinex® HC-1 Planarised PET film
Categories: Polymer; Film; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET)

Material Notes: Products such as Melinex® ST506 can be planerised with a special coating to give surface roughness equivalent to display glass. These films are optically clear and specifically designed for TFT or OLED applications.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 125 - 175 microns
 
Mechanical PropertiesOriginal ValueComments
Flexural Strength 137.9 MPa
Coefficient of Friction 0.60
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+8 - 1.00e+12 ohm-cm
Surface Resistivity per Square 1.00e+8 ohm
Dielectric Constant 2.9
Dielectric Strength 118 kV/mm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 18.0 µm/m-°C
Melting Point 265 °C
Shrinkage 0.10 %
 
Optical PropertiesOriginal ValueComments
Haze 0.0050 %
Transmission, Visible 91.5 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Eastman 9921 PET Film
Chengdu Polyster PET Film PET Films/Sheets
Eastman 9921P PET Film
Eastman 9921W PET Film
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced

PFLEXSM14 / 179530

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.