TPE-S, Shore A79, natural, modified for good adhesion to PBT and PBT blends, among others. KEBAFLEX – H / SPBT 70 A.02 natural was specially developed for outdoor automotive use (UV stabilization) and has optimized demolding behavior. Properties: flexible, good haptics, adhesion modified, High weather resistance, semi-crystalline, soft Typical areas of application: Sealing elements, Seals, Spring elements, Handles, Haptic components Industries: Automotive, Electrical and electronics industry, Household appliances, Industry, Mechanical Engineering, Furniture industry, Sports & Recreation Information provided by BARLOG plastics GmbH. |